Acetylene - Thermophysical Properties
Molecular Weight 26.04
Specific Gravity 0.90
Specific Volume (ft3/lb, m3/kg) 14.9, 0.93
Density of liquid at atmospheric pressure (lb/ft3, kg/m3) 43.0, 693
Absolute Viscosity (lbm/ft s, centipoises) 6.72×10-6, 0.01
Sound velocity in gas (m/s) 343
Specific Heat - cp - (Btu/lb oF or cal/g oC, J/kgK) 0.40, 1674
Specific Heat Ratio - cp/cv 1.25
Gas constant - R - (ft lb/lb oR, J/kg oC) 59.3, 319
Thermal Conductivity (Btu/hr ft oF, W/moC) 0.014, 0.024
Boiling Point - saturation pressure 14.7 psia and 760 mm Hg - (oF, oC) -103, -75
Latent Heat of Evaporation at boiling point (Btu/lb, J/kg) 264, 614000
Freezing or Melting Point  at 1 atm (oF, oC) -116, -82.2
Latent Heat of Fusion (Btu/lb, J/kg) 23, 53500
Critical Temperature (oF, oC) 97.1, 36.2
Critical Pressure (psia, MN/m2) 907, 6.25
Flammable yes
Heat of combustion (Btu/ft3, Btu/lb, kJ/kg) 1450, 21600, 50200
  • values at 25 oC (77 oF, 298 K) and atmospheric pressure

See also more about atmospheric pressure, and STP - Standard Temperature and Pressure & NTP - Normal Temperature and Pressure,
as well as Thermophysical properties of: Acetone, Air, Ammonia, Argon, Benzene, Butane, Carbon dioxide, Carbon monoxide, Ethane, Ethanol, Ethylene, Helium, Hydrogen, Hydrogen sulfide, Methane, Methanol, Nitrogen, Oxygen, Pentane, Propane, Toluene, Water and Heavy water, D2O .

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter


















































9.19.10

.
Cookie Settings