US Standard Mesh, sieve sizes and openings:
| Sieve size (mm) | Opening (in) | US Standard Mesh |
|---|---|---|
| 11.2 | 0.438 | 7/16” |
| 6.35 | 0.250 | 1/4” |
| 5.6 | 0.223 | 3.5 |
| 4.75 | 0.187 | 4 |
| 4.0 | 0.157 | 5 |
| 3.35 | 0.132 | 6 |
| 2.80 | 0.110 | 7 |
| 2.36 | 0.0937 | 8 |
| 2.0 | 0.0787 | 10 |
| 1.7 | 0.0661 | 12 |
| 1.4 | 0.0555 | 14 |
| 1.18 | 0.0469 | 16 |
| 1.0 | 0.0394 | 18 |
| 0.841 | 0.0331 | 20 |
| 0.71 | 0.0278 | 25 |
| 0.595 | 0.0232 | 30 |
| 0.50 | 0.0197 | 35 |
| 0.400 | 0.0165 | 40 |
| 0.355 | 0.0139 | 45 |
| 0.30 | 0.0117 | 50 |
| 0.250 | 0.0098 | 60 |
| 0.210 | 0.0083 | 70 |
| 0.177 | 0.0070 | 80 |
| 0.149 | 0.0059 | 100 |
| 0.125 | 0.0049 | 120 |
| 0.105 | 0.0041 | 140 |
| 0.088 | 0.0035 | 170 |
| 0.074 | 0.0029 | 200 |
| 0.063 | 0.0024 | 230 |
| 0.053 | 0.0021 | 270 |
| 0.044 | 0.0017 | 325 |
| 0.037 | 0.0015 | 400 |
| 0.025 | 0.0010 | 500 |
| 0.020 | 0.0008 | 632 |
Download and print Particle Diameter vs. Mesh Size Chart
Mesh is used to Particle size and the particle-size distribution of a granular material.
Related Topics
• Miscellaneous
Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.
Related Documents
Conveyors - Capacities
Calculate conveyor capacities.
Conveyors - Load & Power Consumption
Conveyor required power consumption vs. load.
Conveyors - Maximum Inclination vs. Product
Maximum conveyor inclination slopes for typical products.
Gravel - Cover Area
Gravel aggregate covering area.
Mesh Sizes vs. Particle Diameters
Strainers and filters - mesh size vs. particle diameter opening size.
Pneumatic Powder and Solid Transport Systems
Pneumatic transport systems used to move powder and other solid products.
Pneumatic Powder Transport
An introduction to pneumatic transport of powders.
Pneumatic Transport - Solids and Particle Size
Particle sizes for common products like coal, sand, ash and more.
Pneumatic Transport and Conveying - Carrying Velocities
Recommended air velocity for pneumatic transport of products like cement, coal, flour and more.
Slurry Transports - Minimum Flow Velocities
Flow velocities in slurry transport systems to avoid settling of solids.
Stockpile Volumes
Volume of natural stockpiles - cubic feet, yard, metre and decimetre.
Surface Roughness vs. Abrasive Grain Size
U.S. mesh size vs. surface roughness.
Surface Roughness vs. Mechanical Processing
Mechanical production methods and their surface roughness.