| Surface Roughness Ra (μm) | Abrasive Grain Size (U.S. mesh size) |
|---|---|
| 0.7 - 1.1 | 46 |
| 0.35 - 0.7 | 60 |
| 0.2 - 0.4 | 80 |
| 0.17 - 0.25 | 100 |
| 0.14 - 0.2 | 120 |
| 0.12 - 0.17 | 150 |
| 0.1 - 0.14 | 180 |
| 0.08 - 0.12 | 220 |
Related Topics
• Miscellaneous
Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.
Related Documents
Building Tolerances
Typical tolerances for floors, walls, columns and more.
Grit Size vs. Surface Roughness
Comparing sandpaper grit size and surface roughness.
Machine Processing - Tolerance Grades
Machine processing and tolerance grades.
Manning’s Roughness Coefficients for Open Channel Flow
Manning's roughness coefficients for some common materials.
Sieve Sizes vs. Mesh Designations
US commercial sieve sizes vs. mesh designations.
Surface Roughness vs. Mechanical Processing
Mechanical production methods and their surface roughness.