Malleable Iron Threaded Fittings - Pressure vs. Temperature Rating
This Standard for threaded malleable iron fittings Classes 150, and 300 provides requirements for the following:
- (a) pressure-temperature ratings
- (b) size and method of designating openings of reducing fittings
- (c) marking
- (d) materials
- (e) dimensions and tolerances
- (f) threading
- (g) coatings
Pressure-temperature ratings can be found in the table below:
| Temperature | Pressure-Temperature ratings for malleable iron threaded fittings (psig) | ||||
|---|---|---|---|---|---|
| Class | |||||
| 150 | 300 | ||||
| 1/4 - 1 inches | 1 1/4 - 2 inches | 2 1/2 - 3 inches | |||
| (oF) | (oC) | ||||
| -20 to 150 | -29 to 66 | 300 | 2000 | 1500 | 1000 |
| 200 | 93 | 265 | 1785 | 1350 | 910 |
| 250 | 121 | 225 | 1575 | 1200 | 825 |
| 300 | 149 | 185 | 1360 | 1050 | 735 |
| 350 | 177 | 150 | 1150 | 900 | 650 |
| 400 | 204 | - | 935 | 750 | 560 |
| 450 | 232 | - | 725 | 600 | 475 |
| 500 | 260 | - | 510 | 450 | 385 |
| 550 | 288 | - | 300 | 300 | 300 |
- 1 psi = 0.0689 bar = 6.89 kPa
Related Topics
• Pressure Ratings of Pipes and Fittings
Pressure ratings of pipes and tubes and their fittings - carbon steel , stainless steel, plastic, copper and more.
Related Documents
ASME/ANSI B16 Standards for Pipes and Fittings
The ASME B16 standards covers pipes and fittings in cast iron , cast bronze, wrought copper and steel.
BSi - Pipe, Tube and Fittings Standards and Specifications
British standards and specifications for pipe, tube and fittings.
Cast Iron Threaded Pipe Fittings - Working Pressures vs. Temperature
Maximum working pressures for cast iron threaded pipe fittings according ANSI B16.4.
DIN - Pipe, Tube and Fittings Standards and Specifications
Deutsches Institut für Normung - DIN - pipe, tube and fittings standards and specifications.
PN Pressure Ratings for Flanges: Specifications & Standards
Pressure numbers (PN) vs. flange class designations.