Commercial Pipes Properties
Dimensions and properties of commercial pipes:
| Nominal Diameter (mm) | Schedule | Outside Diameter (mm) | Wall Thickness (mm) | Inside Diameter (mm) | Inside Area (cm2) | Pipe Weight (kg/m) | |
|---|---|---|---|---|---|---|---|
| 3 | 10S | 10.3 | 1.2446 | 7.811 | 0.48 | 0.27 | |
| Std | 40 | 10.3 | 1.7272 | 6.846 | 0.37 | 0.36 | |
| XS | 80 | 10.3 | 2.413 | 5.474 | 0.25 | 0.47 | |
| 6 | 10S | 13.7 | 1.651 | 10.398 | 0.85 | 0.49 | |
| Std | 40 | 13.7 | 2.235 | 9.23 | 0.67 | 0.63 | |
| XS | 80 | 13.7 | 3.023 | 7.654 | 0.46 | 0.79 | |
| 10 | 10S | 17.145 | 1.651 | 13.843 | 1.51 | 0.63 | |
| Std | 40 | 17.145 | 2.311 | 12.523 | 1.23 | 0.84 | |
| XS | 80 | 17.145 | 3.2 | 10.745 | 0.91 | 1.1 | |
| 15 | 5S | 21.336 | 1.651 | 18.034 | 2.55 | 0.8 | |
| 10S | 21.336 | 2.108 | 17.12 | 2.30 | 1.0 | ||
| Std | 40 | 21.336 | 2.769 | 15.798 | 1.96 | 1.27 | |
| XS | 80 | 21.336 | 3.734 | 13.868 | 1.51 | 1.62 | |
| 160 | 21.336 | 4.75 | 11.836 | 1.1 | 1.94 | ||
| XXS | 21.336 | 7.468 | 6.4 | 0.32 | 2.55 | ||
| 20 | 5S | 26.67 | 1.651 | 23.368 | 4.29 | 1.02 | |
| 10S | 26.67 | 2.108 | 22.454 | 3.96 | 1.27 | ||
| Std | 40 | 26.67 | 2.87 | 20.93 | 3.44 | 1.68 | |
| XS | 80 | 26.67 | 3.912 | 18.846 | 2.79 | 2.19 | |
| 160 | 26.67 | 5.534 | 15.596 | 1.91 | 2.88 | ||
| XXS | 26.67 | 7.823 | 11.024 | 0.95 | 3.63 | ||
| 25 | 5S | 33.401 | 1.651 | 30.099 | 7.12 | 1.29 | |
| 10S | 33.401 | 2.769 | 27.863 | 6.10 | 2.09 | ||
| Std | 40 | 33.401 | 3.378 | 26.645 | 5.58 | 2.49 | |
| XS | 80 | 33.401 | 4.547 | 24.307 | 4.64 | 3.23 | |
| 160 | 33.401 | 6.35 | 20.701 | 3.37 | 4.23 | ||
| XXS | 33.401 | 9.093 | 15.215 | 1.82 | 5.44 | ||
| 32 | 5S | 42.164 | 1.651 | 38.862 | 11.86 | 1.65 | |
| 10S | 42.164 | 2.769 | 36.626 | 10.54 | 2.68 | ||
| Std | 40 | 42.164 | 3.556 | 35.052 | 9.65 | 3.38 | |
| XS | 80 | 42.164 | 4.851 | 32.462 | 8.28 | 4.45 | |
| 160 | 42.164 | 6.35 | 29.464 | 6.82 | 5.59 | ||
| XXS | 42.164 | 9.703 | 22.758 | 4.07 | 7.747 | ||
| 40 | 5S | 48.26 | 1.651 | 44.958 | 15.88 | 1.89 | |
| 10S | 48.26 | 2.769 | 42.722 | 14.34 | 3.1 | ||
| Std | 40 | 48.26 | 3.683 | 40.894 | 13.13 | 4.04 | |
| XS | 80 | 48.26 | 5.08 | 38.1 | 11.40 | 5.4 | |
| 160 | 48.26 | 7.137 | 33.986 | 9.07 | 7.22 | ||
| XXS | 48.26 | 10.16 | 27.94 | 6.13 | 9.52 | ||
| 48.26 | 13.335 | 21.59 | 3.66 | 11.46 | |||
| 48.26 | 15.875 | 16.51 | 2.14 | 12.65 | |||
| 50 | 5S | 60.325 | 1.651 | 57.023 | 25.54 | 2.38 | |
| 10S | 60.325 | 2.769 | 54.787 | 23.58 | 3.92 | ||
| Std | 40 | 60.325 | 3.912 | 52.501 | 21.65 | 5.43 | |
| XS | 80 | 60.325 | 5.537 | 49.251 | 19.055 | 7.46 | |
| 160 | 60.325 | 8.712 | 42.901 | 14.46 | 11.06 | ||
| XXS | 60.325 | 11.074 | 38.177 | 11.45 | 13.42 | ||
| 60.325 | 14.275 | 31.775 | 7.93 | 16.17 | |||
| 60.325 | 17.45 | 25.425 | 5.08 | 18.40 | |||
| 65 | 5S | 73.025 | 2.108 | 68.809 | 37.19 | 3.68 | |
| 10S | 73.025 | 3.048 | 66.929 | 35.18 | 5.25 | ||
| Std | 40 | 73.025 | 5.156 | 62.713 | 30.89 | 8.61 | |
| XS | 80 | 73.025 | 7.01 | 59.005 | 27.34 | 11.38 | |
| 160 | 73.025 | 9.525 | 53.975 | 22.88 | 14.88 | ||
| XXS | 73.025 | 14.021 | 44.983 | 15.89 | 20.35 | ||
| 73.025 | 17.145 | 38.735 | 11.78 | 23.56 | |||
| 73.025 | 20.32 | 32.385 | 8.24 | 26.34 | |||
| 80 | 5S | 88.9 | 2.108 | 84.684 | 56.32 | 4.50 | |
| 10S | 88.9 | 3.048 | 82.804 | 53.85 | 6.44 | ||
| Std | 40 | 88.9 | 5.486 | 77.928 | 47.70 | 11.26 | |
| XS | 80 | 88.9 | 7.62 | 73.66 | 42.61 | 15.23 | |
| 160 | 88.9 | 11.1 | 66.7 | 34.94 | 21.24 | ||
| XXS | 88.9 | 15.24 | 58.42 | 26.81 | 27.61 | ||
| 88.9 | 18.415 | 52.07 | 21.29 | 31.93 | |||
| 88.9 | 21.59 | 45.72 | 16.42 | 35.74 | |||
| 90 | 5S | 101.6 | 2.108 | 97.384 | 74.49 | 5.16 | |
| 10S | 101.6 | 3.048 | 95.504 | 71.64 | 7.39 | ||
| Std | 40 | 101.6 | 5.74 | 90.12 | 63.79 | 13.53 | |
| XS | 80 | 101.6 | 8.077 | 85.446 | 57.34 | 18.58 | |
| XXS | 101.6 | 16.154 | 69.292 | 37.71 | 33.95 | ||
| 100 | 5S | 114.3 | 2.108 | 110.084 | 95.18 | 5.82 | |
| 10S | 114.3 | 3.048 | 108.204 | 91.96 | 8.34 | ||
| 114.3 | 4.775 | 104.75 | 86.18 | 12.86 | |||
| Std | 40 | 114.3 | 6.02 | 102.6 | 82.13 | 16.03 | |
| XS | 80 | 114.3 | 8.56 | 97.18 | 74.17 | 22.3 | |
| 120 | 114.3 | 11.1 | 92.1 | 66.62 | 28.2 | ||
| 114.3 | 12.7 | 88.9 | 62.07 | 31.7 | |||
| 160 | 114.3 | 13.487 | 87.326 | 59.89 | 33.4 | ||
| XXS | 114.3 | 17.12 | 80.06 | 50.34 | 40.9 | ||
| 114.3 | 20.32 | 73.66 | 42.61 | 47 | |||
| 114.3 | 23.495 | 67.31 | 35.58 | 52.5 | |||
| 125 | 5S | 141.3 | 2.769 | 135.762 | 144.76 | 9.44 | |
| 10S | 141.3 | 3.404 | 134.492 | 142.06 | 11.5 | ||
| Std | 40 | 141.3 | 6.553 | 128.194 | 129.07 | 21.7 | |
| XS | 80 | 141.3 | 9.525 | 122.25 | 117.38 | 30.9 | |
| 120 | 141.3 | 12.7 | 115.9 | 105.50 | 40.2 | ||
| 160 | 141.3 | 15.875 | 109.55 | 94.26 | 49 | ||
| XXS | 141.3 | 19.05 | 103.2 | 83.65 | 57.3 | ||
| 141.3 | 22.225 | 96.85 | 73.67 | 65.1 | |||
| 141.3 | 25.4 | 90.5 | 64.33 | 72.4 | |||
| 150 | 5S | 168.275 | 2.769 | 162.737 | 208 | 11.3 | |
| 10S | 168.275 | 3.404 | 161.467 | 204.77 | 13.8 | ||
| 168.275 | 5.563 | 157.149 | 193.96 | 22.3 | |||
| Std | 40 | 168.275 | 7.122 | 154.051 | 186.39 | 28.2 | |
| XS | 80 | 168.275 | 10.973 | 146.329 | 168.17 | 42.5 | |
| 120 | 168.275 | 14.275 | 139.725 | 153.33 | 54.1 | ||
| 160 | 168.275 | 18.237 | 131.801 | 136.44 | 67.3 | ||
| XXS | 168.275 | 21.946 | 124.383 | 121.51 | 79 | ||
| 168.275 | 25.4 | 117.475 | 108.39 | 89.3 | |||
| 168.275 | 28.575 | 111.125 | 96.99 | 98.2 | |||
| 200 | 5S | 219.075 | 2.769 | 213.537 | 358.12 | 14.7 | |
| 10S | 219.075 | 3.759 | 211.557 | 351.52 | 19.9 | ||
| 219.075 | 5.563 | 207.949 | 339.63 | 29.2 | |||
| 20 | 219.075 | 6.35 | 206.375 | 334.51 | 33.2 | ||
| 30 | 219.075 | 7.036 | 205.003 | 330.07 | 36.7 | ||
| Std | 40 | 219.075 | 8.179 | 202.717 | 322.75 | 42.4 | |
| 60 | 219.075 | 10.312 | 198.451 | 309.31 | 52.9 | ||
| XS | 80 | 219.075 | 12.7 | 193.675 | 294.60 | 64.5 | |
| 100 | 219.075 | 15.062 | 188.951 | 280.41 | 75.6 | ||
| 120 | 219.075 | 18.237 | 182.601 | 261.88 | 90.1 | ||
| 140 | 219.075 | 20.625 | 177.825 | 248.36 | 100.7 | ||
| 160 | 219.075 | 23.012 | 173.051 | 235.20 | 111 | ||
| 219.075 | 25.4 | 168.275 | 222.40 | 121 | |||
| 219.075 | 28.575 | 161.925 | 205.93 | 133.9 | |||
| 250 | 5S | 273.05 | 3.404 | 266.242 | 556.73 | 22.6 | |
| 10S | 273.05 | 4.191 | 264.668 | 550.17 | 27.7 | ||
| 273.05 | 5.563 | 261.924 | 538.82 | 36.6 | |||
| 20 | 273.05 | 6.35 | 260.35 | 532.36 | 41.7 | ||
| 30 | 273.05 | 7.798 | 257.454 | 520.58 | 50.9 | ||
| Std | 40 | 273.05 | 9.271 | 254.508 | 508.74 | 60.1 | |
| XS | 60 | 273.05 | 12.7 | 247.65 | 481.69 | 81.3 | |
| 80 | 273.05 | 15.062 | 242.926 | 463.49 | 95.6 | ||
| 100 | 273.05 | 18.237 | 236.576 | 439.57 | 114.3 | ||
| 120 | 273.05 | 21.412 | 230.226 | 416.29 | 132.5 | ||
| 273.05 | 22.225 | 228.6 | 410.43 | 137.1 | |||
| 140 | 273.05 | 25.4 | 222.25 | 387.95 | 154.7 | ||
| 160 | 273.05 | 28.575 | 215.9 | 366.10 | 171.8 | ||
| 273.05 | 31.75 | 209.55 | 344.88 | 188.4 | |||
| 273.05 | 38.1 | 196.85 | 304.34 | 220.2 | |||
| 300 | 5S | 323.85 | 3.962 | 315.926 | 783.90 | 31.2 | |
| 10S | 323.85 | 4.572 | 314.706 | 777.86 | 35.9 | ||
| 20 | 323.85 | 6.35 | 311.15 | 760.4 | 49.6 | ||
| 30 | 323.85 | 8.382 | 307.086 | 740.6 | 65 | ||
| Std | 323.85 | 9.525 | 304.8 | 729.7 | 76.6 | ||
| 40 | 323.85 | 10.312 | 303.226 | 722.1 | 79.5 | ||
| XS | 323.85 | 12.7 | 298.45 | 699.6 | 97.2 | ||
| 60 | 323.85 | 14.275 | 295.3 | 684.9 | 108.7 | ||
| 80 | 323.85 | 17.45 | 288.95 | 655.7 | 131.5 | ||
| 323.85 | 19.05 | 285.75 | 641.3 | 142.8 | |||
| 100 | 323.85 | 21.412 | 271.026 | 620.3 | 159.3 | ||
| 323.85 | 22.225 | 279.4 | 613.1 | 164.9 | |||
| 120 | 323.85 | 25.4 | 273.05 | 585.6 | 186.4 | ||
| 140 | 323.85 | 28.575 | 266.7 | 558.6 | 207.5 | ||
| 323.85 | 31.75 | 260.35 | 532.4 | 228.1 | |||
| 160 | 323.85 | 33.325 | 257.2 | 519.6 | 238.1 | ||
| 350 | 5S | 355.6 | 3.962 | 347.676 | 949.4 | 34.3 | |
| 10S | 355.6 | 4.775 | 346.05 | 940.5 | 41.2 | ||
| 355.6 | 5.334 | 344.932 | 934.5 | 46 | |||
| 355.6 | 5.563 | 344.474 | 932 | 47.9 | |||
| 10 | 355.6 | 6.35 | 342.9 | 923.5 | 54.5 | ||
| 355.6 | 7.137 | 341.326 | 915 | 61.2 | |||
| 20 | 355.6 | 7.925 | 339.75 | 906.6 | 67.8 | ||
| 355.6 | 8.738 | 338.124 | 897.9 | 74.5 | |||
| Std | 30 | 355.6 | 9.525 | 336.55 | 889.6 | 81.1 | |
| 40 | 355.6 | 11.1 | 333.4 | 873 | 94.1 | ||
| 355.6 | 11.913 | 331.774 | 864.5 | 100.7 | |||
| XS | 355.6 | 12.7 | 330.2 | 856.3 | 107.1 | ||
| 60 | 355.6 | 15.062 | 325.476 | 832 | 126.2 | ||
| 355.6 | 15.875 | 323.85 | 823.7 | 132.7 | |||
| 80 | 355.6 | 19.05 | 317.5 | 791.7 | 157.7 | ||
| 100 | 355.6 | 23.8 | 308 | 745.1 | 194.3 | ||
| 120 | 355.6 | 27.762 | 300.076 | 707.2 | 223.9 | ||
| 140 | 355.6 | 31.75 | 292.1 | 670.1 | 252.9 | ||
| 160 | 355.6 | 35.712 | 284.176 | 634.3 | 281 | ||
| 400 | 5S | 406.4 | 4.191 | 398.018 | 1244.2 | 41.5 | |
| 10S | 406.4 | 4.775 | 396.85 | 1236.9 | 47.2 | ||
| 10 | 406.4 | 6.35 | 393.7 | 1217.4 | 62.5 | ||
| 20 | 406.4 | 7.925 | 390.55 | 1198 | 77.6 | ||
| Std | 30 | 406.4 | 9.525 | 387.35 | 1178.4 | 93 | |
| XS | 40 | 406.4 | 12.7 | 381 | 1140.1 | 123 | |
| 60 | 406.4 | 16.662 | 373.076 | 1093.2 | 159.7 | ||
| 80 | 406.4 | 21.441 | 363.518 | 1037.9 | 203 | ||
| 100 | 406.4 | 26.187 | 354.026 | 984.4 | 245 | ||
| 120 | 406.4 | 30.937 | 344.526 | 932.3 | 285.7 | ||
| 140 | 406.4 | 36.5 | 333.4 | 873 | 332.1 | ||
| 160 | 406.4 | 40.462 | 325.476 | 832 | 364.2 | ||
| 450 | 5S | 457.2 | 4.191 | 448.818 | 1582.1 | 46.7 | |
| 10S | 457.2 | 4.775 | 447.65 | 1573.9 | 53.1 | ||
| 10 | 457.2 | 6.35 | 444.5 | 1551.8 | 70.4 | ||
| 20 | 457.2 | 7.925 | 441.35 | 1529.9 | 87.6 | ||
| Std | 457.2 | 9.525 | 438.15 | 1507.8 | 104.9 | ||
| 30 | 457.2 | 11.1 | 435 | 1486.2 | 121.8 | ||
| XS | 457.2 | 12.7 | 431.8 | 1464.4 | 138.8 | ||
| 40 | 457.2 | 14.275 | 428.65 | 1443.1 | 155.5 | ||
| 60 | 457.2 | 19.05 | 419.1 | 1379.5 | 205.3 | ||
| 80 | 457.2 | 23.8 | 409.6 | 1317.7 | 253.7 | ||
| 100 | 457.2 | 29.362 | 398.476 | 1247.1 | 309 | ||
| 120 | 457.2 | 34.925 | 387.35 | 1178.4 | 362.7 | ||
| 140 | 457.2 | 39.675 | 377.85 | 1121.3 | 407.4 | ||
| 160 | 457.2 | 45.237 | 366.726 | 1056.3 | 458.4 | ||
| 500 | 5S | 508 | 4.775 | 498.45 | 1951.3 | 59.1 | |
| 10S | 508 | 5.537 | 496.926 | 1939.4 | 68.4 | ||
| 10 | 508 | 6.35 | 495.3 | 1926.8 | 78.3 | ||
| Std | 20 | 508 | 9.525 | 488.95 | 1877.7 | 116.8 | |
| XS | 30 | 508 | 12.7 | 482.6 | 1829.2 | 154.7 | |
| 40 | 508 | 15.062 | 477.876 | 1793.6 | 182.6 | ||
| 60 | 508 | 20.625 | 466.75 | 1711 | 247.2 | ||
| 508 | 22.225 | 463.55 | 1687.7 | 265.5 | |||
| 80 | 508 | 26.187 | 455.625 | 1630.5 | 310.3 | ||
| 100 | 508 | 32.537 | 442.926 | 1540.8 | 380.5 | ||
| 120 | 508 | 38.1 | 431.8 | 1464.4 | 440.3 | ||
| 140 | 508 | 44.45 | 419.1 | 1379.5 | 506.8 | ||
| 160 | 508 | 49.987 | 408.026 | 1307.6 | 563.1 | ||
| 550 | 5S | 558.8 | 4.775 | 549.25 | 2369.4 | 65.1 | |
| 10S | 558.8 | 5.537 | 547.726 | 2356.2 | 75.3 | ||
| 10 | 558.8 | 6.35 | 546.1 | 2342.3 | 86.3 | ||
| Std | 20 | 558.8 | 9.525 | 539.75 | 2288.1 | 128.7 | |
| XS | 30 | 558.8 | 12.7 | 533.4 | 2234.6 | 170.6 | |
| 558.8 | 15.875 | 527.05 | 2181.7 | 212 | |||
| 558.8 | 19.05 | 520.7 | 2129.4 | 252.9 | |||
| 60 | 558.8 | 22.225 | 514.35 | 2077.8 | 293.3 | ||
| 80 | 558.8 | 28.575 | 501.65 | 1976.5 | 372.7 | ||
| 100 | 558.8 | 34.925 | 488.95 | 1877.7 | 450 | ||
| 120 | 558.8 | 41.275 | 476.25 | 1781.4 | 525.4 | ||
| 140 | 558.8 | 47.625 | 463.55 | 1687.7 | 598.8 | ||
| 160 | 558.8 | 53.975 | 450.85 | 1596.5 | 670.2 | ||
| 600 | 10 | 609.6 | 6.35 | 596.9 | 2798.3 | 94.2 | |
| Std | 20 | 609.6 | 9.525 | 590.55 | 2739.1 | 140.6 | |
| XS | 609.6 | 12.7 | 584.2 | 2680.5 | 186.5 | ||
| 30 | 609.6 | 14.275 | 581.05 | 2651.7 | 209.0 | ||
| 609.6 | 15.875 | 577.85 | 2622.5 | 231.8 | |||
| 40 | 609.6 | 17.45 | 574.7 | 2594.0 | 254.1 | ||
| 609.6 | 19.05 | 571.5 | 2565.2 | 276.7 | |||
| 5S | 609.6 | 5.537 | 598.526 | 2813.6 | 82.3 | ||
| 609.6 | 22.225 | 565.15 | 2508.5 | 31.1 | |||
| 60 | 609.6 | 24.587 | 560.426 | 2466.8 | 353.8 | ||
| 80 | 609.6 | 30.937 | 547.726 | 2356.2 | 440.3 | ||
| 100 | 609.6 | 38.887 | 531.826 | 221.4 | 545.9 | ||
| 120 | 609.6 | 46.025 | 517.55 | 2103.7 | 638 | ||
| 140 | 609.6 | 52.375 | 504.85 | 2001.8 | 717.8 | ||
| 160 | 609.6 | 59.512 | 490.576 | 1890.2 | 805.2 | ||
| 650 | 660.4 | 6.35 | 647.7 | 3294.9 | 102.2 | ||
| 10 | 660.4 | 7.925 | 644.55 | 3262.9 | 127.2 | ||
| Std | 660.4 | 9.525 | 641.35 | 3230.6 | 152.5 | ||
| XS | 20 | 660.4 | 12.7 | 635 | 3166.9 | 202.3 | |
| 660.4 | 15.875 | 628.65 | 3103.9 | 251.7 | |||
| 660.4 | 19.05 | 622.3 | 3041.5 | 300.5 | |||
| 660.4 | 22.225 | 615.95 | 2979.8 | 348.9 | |||
| 660.4 | 25.4 | 609.6 | 2918.6 | 396.7 | |||
| 660.4 | 28.575 | 603.25 | 2858.2 | 444.1 | |||
| 700 | 711.2 | 6.35 | 698.5 | 3832 | 110.1 | ||
| 10 | 711.2 | 7.925 | 695.35 | 3797.5 | 137.1 | ||
| Std | 711.2 | 9.525 | 692.15 | 3762.6 | 164.4 | ||
| XS | 20 | 711.2 | 12.7 | 685.8 | 3693.9 | 218.2 | |
| 30 | 711.2 | 15.875 | 679.45 | 3625.8 | 271.5 | ||
| 711.2 | 19.05 | 673.1 | 3558.4 | 324.3 | |||
| 711.2 | 22.225 | 666.75 | 3491.5 | 376.6 | |||
| 711.2 | 25.4 | 660.4 | 3425.4 | 428.4 | |||
| 711.2 | 28.575 | 654.05 | 3359.8 | 479.8 | |||
| 750 | 5S | 762 | 6.35 | 749.3 | 4409.6 | 118.0 | |
| 10 | 762 | 7.925 | 746.15 | 4372.6 | 147.0 | ||
| Std | 762 | 9.525 | 742.95 | 4335.2 | 176.3 | ||
| XS | 20 | 762 | 12.7 | 736.6 | 4261.4 | 234.1 | |
| 30 | 762 | 15.875 | 730.25 | 4188.3 | 291.3 | ||
| 40 | 762 | 19.05 | 723.9 | 4115.7 | 348.1 | ||
| 762 | 22.225 | 717.55 | 4043.9 | 404.4 | |||
| 762 | 25.4 | 711.2 | 3972.6 | 460.2 | |||
| 762 | 28.575 | 704.85 | 3902 | 515.5 | |||
| 800 | 812.8 | 6.35 | 800.1 | 5027.8 | 125.9 | ||
| 10 | 812.8 | 7.925 | 796.95 | 4988.3 | 156.9 | ||
| Std | 812.8 | 9.525 | 793.75 | 4948.3 | 188.2 | ||
| XS | 20 | 812.8 | 12.7 | 787.4 | 4869.5 | 249.9 | |
| 30 | 812.8 | 15.875 | 781.05 | 4791.2 | 311.2 | ||
| 40 | 812.8 | 14.475 | 777.85 | 4752.1 | 341.8 | ||
| 812.8 | 19.05 | 774.7 | 4713.7 | 371.9 | |||
| 812.8 | 22.225 | 768.35 | 4636.7 | 432.2 | |||
| 812.8 | 25.4 | 762 | 4560.4 | 491.9 | |||
| 812.8 | 28.575 | 755.65 | 4484.7 | 551.2 | |||
| 850 | 863.6 | 6.35 | 850.9 | 5686.6 | 133.9 | ||
| 10 | 863.6 | 7.925 | 847.75 | 5644.5 | 166.8 | ||
| Std | 863.6 | 9.525 | 844.55 | 5602.0 | 200.1 | ||
| XS | 20 | 863.6 | 12.7 | 838.2 | 5518.1 | 265.8 | |
| 30 | 863.6 | 15.875 | 831.85 | 5434.8 | 331 | ||
| 40 | 863.6 | 17.475 | 828.65 | 5393.0 | 363.7 | ||
| 863.6 | 19.05 | 825.5 | 5352.1 | 395.7 | |||
| 863.6 | 22.225 | 819.15 | 5270.1 | 459.9 | |||
| 863.6 | 25.4 | 812.8 | 5188.7 | 523.6 | |||
| 863.6 | 28.575 | 806.45 | 5107.9 | 586.9 | |||
| 900 | 914.4 | 6.35 | 901.7 | 6385.8 | 141.8 | ||
| 10 | 914.4 | 7.925 | 898.55 | 6341.3 | 176.7 | ||
| Std | 914.4 | 9.525 | 895.35 | 6296.2 | 212 | ||
| XS | 20 | 914.4 | 12.7 | 889 | 6207.2 | 281.7 | |
| 30 | 914.4 | 15.875 | 882.65 | 6118.8 | 350.8 | ||
| 40 | 914.4 | 19.05 | 876.3 | 6031.1 | 419.5 | ||
| 914.4 | 22.225 | 869.95 | 5944.0 | 487.7 | |||
| 914.4 | 25.4 | 863.6 | 5857.5 | 555.4 | |||
| 914.4 | 28.575 | 857.25 | 5771.7 | 622.6 | |||
| 1050 | 1066.8 | 6.35 | 1054.1 | 8726.8 | 165.6 | ||
| Std | 1066.8 | 9.525 | 1047.75 | 8622.0 | 247.7 | ||
| XS | 20 | 1066.8 | 12.7 | 1041.4 | 8517.8 | 329.3 | |
| 30 | 1066.8 | 15.875 | 1035.05 | 8414.2 | 410.3 | ||
| 40 | 1066.8 | 19.05 | 1028.7 | 8311.3 | 490.9 | ||
| 1066.8 | 25.4 | 1016 | 8107.4 | 650.6 | |||
| 1066.8 | 31.75 | 1003.3 | 7905.9 | 808.3 | |||
| 1066.8 | 38.1 | 990.6 | 7707 | 964 | |||
Related Topics
• Dimensions of Pipes and Tubes
Pipe, tube and fittings sizes and dimensions. Inside and outside diameters, weights and more.
Related Documents
ASME/ANSI B36.10/19 - Carbon, Alloy and Stainless Steel Pipe - Dimensions
Pipe sizes, inside and outside diameters, wall thickness, schedules, moment of inertia, transverse area, weight of pipe filled with water - U.S. Customary Units.
Beams Natural Vibration Frequency
Estimate structures natural vibration frequency.