Salt Hydrates - Melting points and Latent Melting Energy
The latent heat of melting salt hydrates can be used for storing energy.
| Salt Hydrate | Melting Point (oC) | Latent Melting Heat (MJ/m3) |
|---|---|---|
| CaCl2 (Calcium Chloride) 6H2O | 29 | 281 |
| Na2SO4 (Sodium Sulfate) 10H2O | 32 | 342 |
| Na2CO3 (Sodium Carbonate) 10H2O | 33 | 360 |
| Na2HPO4 (Dibasic Sodium Orthophosphate) 12H2O | 35 | 205 |
| Na2HPO4 (Dibasic Sodium Orthophosphate) 7H2O | 48 | 302 |
| Na2S2O3 (Sodium Thiosulphate) 5H2O | 48 | 346 |
| Ba(OH)2 (Barium Hydroxide) 8H2O | 78 | 655 |
Related Topics
• Melting and Freezing Points
Melting and freezing points of elements and chemical species at varying conditions.
• Thermodynamics
Work, heat and energy systems.
Related Documents
Aluminum - Melting Points of Binary Eutectic Alloys
Al - Aluminum - binary eutectic alloys and their melting points.
Copper Binary Eutectic Alloys - Melting Points
Cu - Copper - binary eutectic alloys and their melting points.
Energy
Energy is the capacity to do work.
Energy Accumulated in Heated Water - kWh
The amount of thermal energy stored in heated water.
Flywheels - Kinetic Energy
The kinetic energy stored in flywheels - the moment of inertia.
Heat, Work and Energy
Heat vs. work vs. energy.
Kinetic Energy
Energy possessed by an object's motion is kinetic energy.
Potential Energy - Hydropower
Elevation and potential energy in hydropower.
Storing Thermal Heat
Energy stored as sensible heat in different types of materials.