Rigid Aluminum Conduits - RAC
Rigid Aluminum Conduit - RAC (alt. Aluminum Rigid Conduit - ARC) dimensions used in raceways:
| Nominal Conduit Size | Outside Diameter | Inside Diameter | Approx. Installation Weight | Approx. Installation Weight with Conductors | |||||
|---|---|---|---|---|---|---|---|---|---|
| (in) | (mm) | (in) | (mm) | (in) | (mm) | (lbs/100 ft) | (kg/30 m) | (lbs/100 ft) | (kg/30 m) |
| 1/2 | 15 | 0.84 | 21.3 | 0.632 | 16.1 | 27 | 13 | 50 | 23 |
| 3/4 | 20 | 1.05 | 26.7 | 0.836 | 21.2 | 36 | 17 | 77 | 35 |
| 1 | 25 | 1.315 | 33.4 | 1.063 | 27 | 53 | 24 | 119 | 54 |
| 1 1/4 | 32 | 1.66 | 42.2 | 1.394 | 35.4 | 70 | 32 | 187 | 85 |
| 1 1/2 | 40 | 1.9 | 48.3 | 1.624 | 41.2 | 82 | 37 | 242 | 110 |
| 2 | 50 | 2.375 | 60.3 | 2.083 | 52.9 | 116 | 53 | 378 | 171 |
| 2 1/2 | 65 | 2.875 | 73 | 2.489 | 63.2 | 183 | 83 | 557 | 252 |
| 3 | 80 | 3.5 | 88.9 | 3.09 | 78.5 | 239 | 108 | 815 | 370 |
| 3 1/2 | 90 | 4 | 101.6 | 3.57 | 90.7 | 288 | 131 | 1061 | 481 |
| 4 | 100 | 4.5 | 114.3 | 4.05 | 102.9 | 340 | 154 | 1334 | 605 |
| 5 | 125 | 5.563 | 141.3 | 5.073 | 128.9 | 465 | 211 | 2028 | 920 |
| 6 | 150 | 6.625 | 168.3 | 6.093 | 154.8 | 613 | 278 | 2870 | 1302 |
Related Topics
• Electrical
Electrical engineering with units, amps and electrical wiring. Wire gauges, electrical formulas, motors and more.
Related Documents
AWG - Wire Gauge Sizes: Current Ratings, Charts, Measurements, and Conversion Guide
Amp ratings vs. US AWG wire gauge.
AWG Wire Gauge Chart & Table – American Wire Gauge (AWG) Standards
The AWG (American Wire Gauge) wire size chart with detailed specifications on wire diameter, resistance, and ampacity. Find conversions between AWG sizes and metric units for electrical and engineering applications.
Electrical Metal Tubing (EMT) - Conduits
Trade sizes and max. distance between conduit supports.
Intermediate Metal Conduit - IMC
Lighter and lower cost metal conduits.