Materials - Light Reflecting Factors
Some materials and their light reflecting factors:
| Material | Reflection Factor (%) |
|---|---|
| Aluminum coatings, matte | 55 - 56 |
| Aluminum, anodized, matte | 80 - 85 |
| Aluminum, matte | 55 - 75 |
| Aluminum, polished | 65 - 75 |
| Aluminum, pure, highly polished | 80 - 87 |
| Body where no light is reflected (Black body) | 0 |
| Body where all light is reflected | 100 |
| Brick, red | 10 - 15 |
| Chrome, polished | 60 - 70 |
| Concrete, rough | 20 - 30 |
| Copper, highly polished | 70 - 75 |
| Crops | 15 - 24 |
| Forrest | 7 - 14 |
| Granite | 20 - 25 |
| Ice | 32 - 38 |
| Lacquer, pure white | 80 - 85 |
| Limestone | 35 - 55 |
| Marble, polished | 30 - 70 |
| Nickel, highly polished | 50 - 60 |
| Oak, light polished | 25 - 35 |
| Paint, brown | 20 - 30 |
| Paint, dark blue | 15 - 20 |
| Paint, dark green | 15 - 20 |
| Paint, dark red | 15 - 20 |
| Paint, light green | 45 - 55 |
| Paint, light yellow | 60 - 70 |
| Paint, medium grey | 25 - 35 |
| Paint, white | 75 - 85 |
| Paper, white | 70 - 80 |
| Plaster, dark | 15 - 25 |
| Plaster, light | 40 - 45 |
| Plywood, rough | 25 - 40 |
| Sand - dry | 38 - 42 |
| Sand - wet | 22 - 28 |
| Sandstone | 20 - 40 |
| Snow - fresh | 85 |
| Snow - old | 45 |
| Silver, highly polished | 90 - 92 |
| Silvered mirror, behind glass | 80 - 88 |
| Soil - dry | 22 - 34 |
| Soil - dark wet | 7 - 14 |
| Stainless steel | 50 |
| Vitreous Enamel, white | 65 - 75 |
| Water | 7 - 9 |
Albedo is the diffuse reflected solar radiation related to the total solar radiation.
Related Topics
• Miscellaneous
Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.
Related Documents
Absorbed Solar Radiation
Solar radiation absorbed by various materials.
Electromagnetic Spectrum
The electromagnetic spectrum with wavelengths and frequencies.
Illuminance - Recommended Light Levels
Working activities and light levels - required illuminance.
LENI - Lighting Energy Numeric Indicator
Energy consumption of lighting systems
Ligths - Color Temperatures
Light sources and their color irradiation in degrees Kelvin.
Luminous Efficacy
The visible light produced by light sources.
Optical Distance Law
Geometric dilution of light vs. distance.
Physical Constants
Physical constants - SI Units.
Refractive Index common Liquids, Solids and Gases
Some common liquids, solids, and gases and their refractive indexes.