The European Standard EN 10241 Steel threaded pipe fittings specifies screw threaded fittings made from welded steel or seamless steel tubes, forging and rolled bars.
| Nominal Diameter DN | Nominal Pipe Size NPS | Outside Diameter (mm) |
|---|---|---|
| 6 | 1/8 | 10.3 |
| 8 | 1/4 | 13.7 |
| 10 | 3/8 | 17.1 |
| 15 | 1/2 | 21.3 |
| 20 | 3/4 | 26.7 |
| 25 | 1 | 33.4 |
| 32 | 1 1/4 | 42.2 |
| 40 | 1 1/2 | 48.3 |
| 50 | 2 | 60.3 |
| 65 | 2 1/2 | 73.0 |
| 80 | 3 | 88.9 |
| 100 | 4 | 114.3 |
| 125 | 5 | 139.7 |
| 150 | 6 | 168.3 |
Related Topics
• Dimensions of Pipes and Tubes
Pipe, tube and fittings sizes and dimensions. Inside and outside diameters, weights and more.
• Threads
Thread data - metric, unified, ACME and others.
Related Documents
ANSI Steel Pipes Schedule 80: Dimensions, Sizes, and Specifications
Internal and external diameters, areas, weights, volumes and number of threads for schedule 80 steel pipes.
ASME/ANSI B36.10/19 - Carbon, Alloy and Stainless Steel Pipe - Dimensions
Pipe sizes, inside and outside diameters, wall thickness, schedules, moment of inertia, transverse area, weight of pipe filled with water - U.S. Customary Units.
ASME/ANSI B36.10/19 - Carbon, Alloy and Stainless Steel Pipes - Dimensions - Metric Units
Pipe sizes, inside and outside diameters, wall thickness, schedules, weight and weight of pipe filled with water - Metric Units.
ASTM A53 B Carbon Steel Pipes - Allowable Pressure vs. Schedule and Size
Maximum working pressure of carbon steel pipe at temperature 400oF.
EN 10255 - Non-alloy Steel Tubes for Welding and Threading - Dimensions
Dimensions and weights of steel tubes according BS EN 10255.
Steel Pipes - Heat Loss Diagram
Heat loss from steel pipes and tubes - dimensions 1/2 to 12 inches.
Steel Pipes - Maximum Water Flow Capacities vs. Size
Maximum water flow capacities in steel pipes - pipe dimensions ranging 2 - 24 inches.
Steel Pipes - Weight
Weight of steel pipes and tubes vs. wall thickness.