Welding Neck Flange Bores
Nominal Pipe Size
(inches)
Outside Diameter
(inches)
Inside Diameter (inches)
Light Wall 1)Schedule 20Schedule 30Standard WallSchedule 40Schedule 60
1/2 0.840 0.674 - - 0.622 0.622 -
3/4 1.050 0.884 - - 0.824 0.824 -
1 1.315 1.097 - - 1.049 1.049 -
1 1/4 1.660 1.442 - - 1.380 1.380 -
1 1/2 1.900 1.682 - - 1.610 1.610 -
2 2.375 2.157 - - 2.067 2.067 -
2 1/2 2.875 2.635 - - 2.469 2.469 -
3 3.500 3.260 - - 3.068 3.068 -
3 1/2 4.000 3.760 - - 3.548 3.548 -
4 4.500 4.260 - - 4.026 4.026 -
5 5.563 5.295 - - 5.047 5.047 -
6 6.625 6.357 - - 6.065 6.065 -
8 8.625 8.329 8.125 8.071 7.981 7.981 7.813
10 10.750 10.420 10.250 10.136 10.020 10.020 9.750
12 12.750 12.390 12.250 12.090 12.000 11.938 11.626
14 14.000 13.500 13.376 13.250 13.250 13.124 12.812
16 16.000 15.500 15.376 15.250 15.250 15.000 14.688
18 18.000 17.500 17.376 17.124 17.250 16.876 16.500
20 20.000 19.500 19.250 19.000 19.250 18.812 18.376
24 24.000 23.500 23.250 22.876 23.250 22.624 22.062
30 30.000 29.376 29.000 28.750 29.250 - -
36 36.000 35.376 35.000 34.750 35.250 34.500 -
42 42.000 - - - 41.250 - -
48 48.000 - - - 47.250 - -
  •  1 inch = 25.4 mm

For full table - rotate the screen!

Welding Neck Flange Bores
Nominal Pipe Size
(inches)
Outside Diameter
(inches)
Inside Diameter (inches)
Extra StrongSchedule 80Schedule 100Schedule 120Schedule 140Schedule 160Double Extra Strong
1/2 0.840 0.546 0.546 - - - 0.464 0.252
3/4 1.050 0.742 0.742 - - - 0.612 0.434
1 1.315 0.957 0.957 - - - 0.815 0.599
1 1/4 1.660 1.278 1.278 - - - 1.160 0.896
1 1/2 1.900 1.500 1.500 - - - 1.338 1.100
2 2.375 1.939 1.939 - - - 1.687 1.503
2 1/2 2.875 2.323 2.323 - - - 2.125 1.771
3 3.500 2.900 2.900 - - - 2.624 2.300
3 1/2 4.000 3.364 3.364 - - - - 2.728
4 4.500 3.826 3.826 - 3.624 - 3.438 3.152
5 5.563 4.813 4.813 - 4.563 - 4.313 4.063
6 6.625 5.761 5.761 - 5.501 - 5.187 4.897
8 8.625 7.625 7.625 7.437 7.187 7.001 6.813 6.875
10 10.750 9.750 9.562 9.312 9.062 8.750 8.500 8.750
12 12.750 11.750 11.374 11.062 10.750 10.500 10.126 10.750
14 14.000 13.000 12.500 12.124 11.814 11.500 11.188 -
16 16.000 15.000 14.312 13.938 13.564 13.124 12.812 -
18 18.000 17.000 16.124 15.688 15.250 14.876 14.438 -
20 20.000 19.000 17.938 17.438 17.000 16.500 16.062 -
24 24.000 23.000 21.562 20.938 20.376 19.876 19.312 -
30 30.000 29.000 - - - - - -
36 36.000 35.000 - - - - - -
42 42.000 41.000 - - - - - -
48 48.000 47.000 - - - - - -

1) Stainless steel Schedule 10S diameters are equal to Light Wall in sizes up to 12" and to Schedule 10 above.

Sponsored Links

Related Topics

Related Documents

Sponsored Links

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with the amazing, fun and free SketchUp Make and SketchUp Pro .Add the Engineering ToolBox extension to your SketchUp from the SketchUp Pro Sketchup Extension Warehouse!

Translate
About the Engineering ToolBox!

Privacy

We don't collect information from our users. Only emails and answers are saved in our archive. Cookies are only used in the browser to improve user experience.

Some of our calculators and applications let you save application data to your local computer. These applications will - due to browser restrictions - send data between your browser and our server. We don't save this data.

Google use cookies for serving our ads and handling visitor statistics. Please read Google Privacy & Terms for more information about how you can control adserving and the information collected.

AddThis use cookies for handling links to social media. Please read AddThis Privacy for more information.

Citation

This page can be cited as

  • Engineering ToolBox, (2003). Carbon and Stainless Steel Welding Neck Flange Bores. [online] Available at: https://www.engineeringtoolbox.com/carbon-stainless-steel-flanges-d_351.html [Accessed Day Mo. Year].

Modify access date.

. .

close

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Scientific Online Calculator

Scientific Calculator

2 6

Sponsored Links
.