ISO 4437 - PE Pipes for Gaseous Fuels Supply - Dimensions

Dimmensions of PE pipes for gaseous supply according ISO 4437.

Dimensions of PE pipes for gaseous supply according ISO 4437 Plastics piping systems -- Polyethylene (PE) pipes and fittings for water supply:

ISO 4437 - PE Pipes for Gaseous Fuels Supply - Dimensions
OD
Nominal Size
(mm)
Wall Thickness (mm)
SDR 17SDR 11
16 2.3
20 2.3
25 2.3
32 2.0 3.0
40 2.4 3.7
50 3.0 4.6
63 3.8 5.8
75 4.5 6.8
90 5.4 8.2
110 6.6 10.0
125 7.4 11.4
140 8.3 12.7
160 9.5 14.6
180 10.7 16.4
200 11.9 18.2
225 13.4 20.5
250 14.8 22.7
280 16.6 25.4
315 18.7 28.6
355 21.1 32.2
400 23.7 36.4
450 26.7 40.9
500 29.7 45.5
560 33.2 50.9
630 37.4 57.3

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). ISO 4437 - PE Pipes for Gaseous Fuels Supply - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/ISO-4437-pe-pipes-gaseous-supply-d_2144.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.26.8

.