Engineering ToolBox - Resources, Tools and Basic Information for Engineering and Design of Technical Applications!

ASTM D2513 - Thermoplastic Gas Pipes - Dimensions

Dimensions of thermoplastic pressure pipes.

Dimensions of thermoplastic gas pipes according ASTM D2513 Standard Specification for Thermoplastic Gas Pressure Pipe, Tubing, and Fittings:

CTS (Copper Tube Sized)

ASTM D2513 - Thermoplastic Gas Pipes - Dimensions - CTS (Copper Tube Sized)
Nominal Tubing Size
(CTS)
(in)
Outside Diameter
(in)
Min. Wall Thickness
(in)
1/4 0.375 0.062
3/8 0.500 0.062
1/2 0.625 0.062
1/2 0.625 0.090
1/2 0.625 0.104
3/4 0.875 0.062
3/4 0.875 0.077
3/4 0.875 0.090
1 1.125 0.062
1 1.125 0.090
1 1.125 0.099
1 1.125 0.101
1 1.125 0.121
1 1/4 1.375 0.062
1 1/4 1.375 0.090
1 1/4 1.375 0.121
1 3/4 1.875 0.062
  • 1 inch = 25.4 mm

IPS (Iron Pipe Sized)

IPS (Iron Pipe Sized)

ASTM D2513 - Thermoplastic Gas Pipes - Dimensions - IPS (Iron Pipe Sized)
Nominal Pipe Size
(IPS)
(in)
SDRMin. Wall Thickness
(in)
1/2 0.062
1/2 11.0 0.076
1/2 9.33 0.090
3/4 0.090
3/4 11.0 0.095
3/4 Sch 40 0.113
1 0.90
1 13.5 0.097
1 11.0 0.120
1 9.9 0.133
1 9.33 0.140
1 1/4 0.090
1 1/4 17.0 0.098
1 1/4 13.5

0.123

1 1/4 Sch 40 0.140
1 1/4 11.0 0.151
1 1/4 10.0 0.166
1 1/4 9.33 0.178
1 1/4 6.0 0.277
1 1/2 0.090
1 1/2 17 0.112
1 1/2 13.5 0.141
1 1/2 Sch 40 0.145
1 1/2 11 0.173
2 21 0.113
2 17 0.140
2 Sch 40 0.154
2 13.5 0.176
2 11 0.216
2 9.33 0.255
2 1/2 21 0.137
2 1/2 17 0.169
2 1/2 13.5 0.213
2 1/2 11 0.261
3 21 0.167
3 17 0.206
3 Sch 40 0.216
3 13.5 0.259
3 11.5 0.304
3 11 0.318
3 9.33 0.375
3 1/2 21 0.190
3 1/2 17 0.236
3 1/2 13.5 0.296
3 1/2 11 0.363
4 21 0.214
4 19 0.237
4 17 0.265
4 13.5 0.333
4 11.5 0.391
4 11.0 0.409
4 9.33 0.482
5 21.6 0.258
5 21 0.265
5 17 0.327
5 13.5 0.412
5 11 0.506
6 32.5 0.204
6 26 0.255
6 23.7 0.280
6 21 0.315
6 17 0.390
6 13.5 0.491
6 11.5 0.576
6 11.0 0.602
8 32.5 0.265
8 26 0.332
8 21 0.411
8 17 0.507
8 13.5 0.639
8 11.5 0.750
8 11 0.784
10 32.5 0.331
10 26 0.413
10 21 0.512
10 17 0.632
10 13.5 0.796
10 11.5 0.935
10 11 0.977
12 32.5 0.392
12 26 0.490
12 21 0.607
12 17 0.750
12 13.5 0.944
12 11.5 1.109
12 11 1.159

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). ASTM D2513 - Thermoplastic Gas Pipes - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/ASTM-D2513-thermoplastic-gas-pipes-d_2137.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































4.26.8

.