Wrought and Cast Copper Alloys - Properties Database

A searchable database of properties for wrought and cast copper alloys.

Properties of Wrought and Cast Copper Alloys.

Wrought and Cast Copper Alloys - Properties
PropertyAnnealed CopperCold Rolled or Drawn CopperCast Copper
Tensile strength (psi) 30000 - 40000 32000 - 60000 20000 - 30000
Tensile strength (MPa) 210 - 280 220 - 400 140 - 210
Elongation in 2 in. 25 - 30% 2 - 35% 25 - 45%
Reduction of area 40 - 60% 2 - 4%
Rockwell F hardness max 65 54 - 100
Roclwell 30T hardness max 31 18 - 70