EN 12201 - Polyethylene (PE) Pipes for Water Supply, and for Drainage and Sewerage under Pressure - Dimensions

Dimensions of PE pipes according EN 12201.

Dimensions of PE pipes according EN 12201-2 Plastics piping systems for water supply, and for drainage and sewerage under pressure - Polyethylene (PE). Pipes:

EN 12201 - Polyethylene (PE) Pipes for Water Supply, and for Drainage and Sewerage under Pressure - Dimensions
Nominal Size
(mm)
Nominal Outside Diameter
(mm)
Mean Outside Diameter (mm) 
Min.Max.
16 16 16.0 16.3
20 20 20.0 20.3
25 25 25.0 25.3
32 32 32.0 32.3
40 40 40.0 40.4
50 50 50.0 50.4
63 63 63.0 63.4
75 75 75.0 75.5
90 90 90.0 90.6
110 110 110.0 110.7
125 125 125.0 125.8
140 140 140.0 140.9
160 160 160.0 161.0
180 180 180.0 181.1
200 200 200.0 201.2
225 225 225.0 226.4
250 250 250.0 251.5
280 280 280.0 281.7
315 315 315.0 316.9
355 355 355.0 357.2
400 400 400.0 402.4
450 450 450.0 452.7
500 500 500.0 503.0
560 560 560.0 563.4
630 630 630.0 633.8
710 710 710.0 716.4
800 800 800.0 807.2
900 900 900.0 908.1
1000 1000 1000.0 1009.0
1200 1200 1200.0 1210.8
1400 1400 1400.0 1412.6
1600 1600 1600.0 1614.4
1800 1800 1800.0 1816.2
2000 2000 2000.0 2018.0
2250 2250 2250.0 2270.3
2500 2500 2500.0 2522.5

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2018). EN 12201 - Polyethylene (PE) Pipes for Water Supply, and for Drainage and Sewerage under Pressure - Dimensions . [online] Available at: https://www.engineeringtoolbox.com/EN-12201-PE-polyethylene-pipes-d_2135.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































6.3.17

.