Concrete Slabs - Load Capacities

Load capacity of simply supported concrete slabs.

Load capacities of simply supported concrete slabs:

Concrete Slabs - Load Capacities
Thickness
(mm)
Self Weight
(kg/m2)
Imposed Load
(kg/m2)
Total LoadSpan
(m)
kg/m2kN/m2
100 240 500 740 7.26 2.4
125 300 500 800 7.85 3.0
150 360 500 860 8.44 3.6

Imposed loads varies from approximately 1.5 kN/m2 (153 kg/m2) in domestic buildings to approximately 10 kN/m2 (1053 kg/m2) in heavy industrial areas. 500 kg/m2 is typical for office, storage space and similar.

Related Topics

  • Miscellaneous

    Engineering related topics like Beaufort Wind Scale, CE-marking, drawing standards and more.

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2011). Concrete Slabs - Load Capacities. [online] Available at: https://www.engineeringtoolbox.com/simply-supported-slabs-load-capacity-d_1803.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.