ElementSymbolMelting Point
(oC)
Actinium Ac 1050
Aluminum Al 660.37
Americum Am 994 +- 4
Antimony  Sb 630.74
Argon  A -189.2
Arsenic  As 817 (at 28 atm)
Astatine  At 302
Barium  Ba 725
Berkelium  Bk  
Beryllium  Be 1278 +- 5
Bismuth  Bi 271.3
Boron  B 2079
Bromine  Br -7.2
Cadmium  Cd 320.9
Calcium  Ca 839 +-2
Californium  Cf  
Carbon  C 3652 (sublimates)
Cerium  Ce 798 +- 2
Cesium  Cs 28.4 +- 0.01
Chlorine  Cl -100.98
Chromium  Cr 1857 +- 20
Cobalt  Co 1495
Copper  Cu 1083.4 +- 0.2
Curium  Cm 1340 +- 40
Dysprosium  Dy 1409
Einsteinium  Es  
Erbium  Er 1522
Europium  Eu 822 +- 5
Fermium  Fm  
Fluorine  F -219.62
Francium  Fr 677
Gadolinium  Gd 1311 +- 1
Gallium  Ga 29.78
Germanium  Ge 937.4
Gold  Au 1064.434
Hafnium  Hf 2227 +- 20
Helium  He -272.2 (at 26 atm)
Holmium  Ho 1470
Hydrogen  H -259.14
Indium  In 156.61
Iodine  I 113.5
Iridium  Ir 2410
Iron  Fe 1535
Krypton  Kr -156.6
Lanthanum  La 920 +- 5
Lawrencium  Lw
Lead  Pb 327.502
Lithium  Li 180.54
Lutetium  Lu 1656 +- 5
Magnesium Mg 648.8 +- 0.5
Manganese Mn 1244 +- 2
Mendelevium Md
Mercury Hg -38.87
Molybdenum Mo 2617
Neodymium Nd 1010
Neon Ne -248.67
Neptunium Np 640 +- 1
Nickel Ni 1453
Niobium Nb 2468 +- 10
Nitrogen N -209.86
Nobelium No
Osmium Os 3045 +- 30
Oxygen O -218.4
Palladium Pd 1554
Phosphorus P 44.1
Platinum Pt 1772
Plutonium Pu 641
Polonium Po 254
Potassium K 63.25
Praseodymium Pr 931 +- 4
Promethium Pm 1080
Protactinium Pa 1600
Radium Ra 700
Radon Rn -71
Rhenium Re 3180
Rhodium Rh 1965 +- 3
Rubidium Rb 38.89
Ruthenium Ru 2310
Samarium Sm 1072 +- 5
Scandium Sc 1539
Selenium Se 217
Silicon Si 1410
Silver Ag 961.93
Sodium Na 97.81 +- 0.03
Strontium Sr 769
Sulphur S 112.8
Tantalum Ta 2996
Technetium Tc 2172
Tellurium Te 449.5 +- 0.3
Terbium Tb 1360 +- 4
Thallium Tl 303.5
Thorium Th 1750
Thulium Tm 1545 +- 15
Tin Sn 231.9681
Titanium Ti 1660 +- 10
Tungsten W 3410 +- 20
Uranium U 1132 +- 0.8
Vanadium V 1890 +- 10
Xenon Xe -111.9
Ytterbium Yb 824 +- 5
Yttrium Y 1523

+- 8

Zinc Zn 419.58
Zirconium Zr 1852 +- 2

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2013). Elements - Melting Points. [online] Available at: https://www.engineeringtoolbox.com/elements-melting-points-d_1863.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.