ASTM A270 Sanitary Stainless Steel Tubing - Dimensions

Dimensions of ASTM A270 sanitary steel tubes.

ASTM A270 Sanitary Stainless Steel Tubing - Dimensions
Outside DiameterNominal Wall ThicknessWeight
(in)(mm)(in)(mm)(kg/m)
1/2 12.7 0.065 1.65 0.454
3/4 19.1 0.065 1.65 0.717
1 25.4 0.065 1.65 0.976
1 1/2 38.1 0.065 1.65 1.50
2 50.8 0.065 1.65 2.02
2 1/2 63.5 0.065 1.65 2.54
3 76.2 0.065 1.65 3.06
4 101.6 0.083 2.11 5.23
6 152.4 0.109 2.77 10.32
8 203.2 0.109 2.77

Related Topics

Related Documents

Search

Search is the most efficient way to navigate the Engineering ToolBox.

Engineering ToolBox - SketchUp Extension - Online 3D modeling!

3D Engineering ToolBox Extension to SketchUp - add parametric components to your SketchUp model

Add standard and customized parametric components - like flange beams, lumbers, piping, stairs and more - to your Sketchup model with the Engineering ToolBox - SketchUp Extension - enabled for use with older versions of the amazing SketchUp Make and the newer "up to date" SketchUp Pro . Add the Engineering ToolBox extension to your SketchUp Make/Pro from the Extension Warehouse !

Translate this Page

Translate this page to Your Own Language .

About the Engineering ToolBox!

Privacy Policy

We don't collect information from our users. More about

We use a third-party to provide monetization technologies for our site. You can review their privacy and cookie policy here.

You can change your privacy settings by clicking the following button: .

Citation

This page can be cited as

  • The Engineering ToolBox (2019). ASTM A270 Sanitary Stainless Steel Tubing - Dimensions. [online] Available at: https://www.engineeringtoolbox.com/ASTM-A270-sanitary-stainless-steel-tubing-d_2160.html [Accessed Day Month Year].

Modify the access date according your visit.

3D Engineering ToolBox - draw and model technical applications! 2D Engineering ToolBox - create and share online diagram drawing templates! Engineering ToolBox Apps - mobile online and offline engineering applications!

Unit Converter

















































5.16.12

.