Temperature
- t -
(oC)

Density
- ρ -
(kg/m3)
Specific Heat
- cp -
(kJ/kg K)
Thermal Coductivity
- λ -
(W/m K)
Dynamic Viscosity
10-6
- η -
(Pa s)
Prandtl's no.
0 1435 1.33 0.212 367 2.31
20 1383 1.37 0.199 304 2.09
50 1296 1.48 0.177 234 1.96