Carbon, Alloy and Stainless Steel Pipes - ASME/ANSI B36.10/19

Pipe sizes, inside and outside diameters, wall thickness, schedules, moment of inertia, transverse area, weight of pipe filled with water - U.S. Customary Units

Sponsored Links

The steel pipe data chart below can be used to find pipe sizes, diameters, wall thickness, working pressures and more The chart is based on ASME/ANSI B 36.10 Welded and Seamless Wrought Steel Pipe and ASME/ANSI B36.19 Stainless Steel Pipe.

Regardless of schedule number, pipes of a particular size all have the same outside diameter (not withstanding manufacturing tolerances). As the schedule number increases, the wall thickness increases, and the actual bore is reduced. For example:

Outside Diameter, Identification, Wall Thickness, Inside Diameter

Pipe Size
(inches)
Outside Diameter
(inches)
Identification Wall Thickness
- t -

(inches)
Inside Diameter
- d -

(inches)
Steel Stainless Steel Schedule No.
Iron Pipe Size Schedule No.
1/8 0.405 .
STD
XS
.
40
80
10S
40S
80S
.049
.068
.095
.307
.269
.215
1/4 0.540 .
STD
XS
.
40
80
10S
40S
80S
.065
.088
.119
.410
.364
.302
3/8 0.675 .
STD
XS
.
40
80
10S
40S
80S
.065
.091
.126
.545
.493
.423
1/2 0.840 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.083
.109
.147
.187
.294
.710
.674
.622
.546
.466
.252
3/4
1.050
.
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.083
.113
.154
.219
.308
.920
.884
.824
.742
.612
.434
1 1.315 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.109
.133
.179
.250
.358
1.185
1.097
1.049
.957
.815
.599
1 1/4 1.660 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.109
.140
.191
.250
.382
1.530
1.442
1.380
1.278
1.160
.896
1 1/2 1.900 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.109
.145
.200
.281
.400
1.770
1.682
1.610
1.500
1.338
1.100
2 2.375 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.065
.109
.154
.218
.344
.436
2.245
2.157
2.067
1.939
1.687
1.503
2 1/2 2.875 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.083
.120
.203
.276
.375
.552
2.709
2.635
2.469
2.323
2.125
1.771
3 3.500 .
.
STD
XS
.
XXS
.
.
40
80
160
.
5S
10S
40S
80S
.
.
.083
.120
.216
.300
.438
.600
3.334
3.260
3.068
2.900
2.624
2.300
3 1/2 4.000 .
.
STD
XS
.
.
40
80
5S
10S
40S
80S
.083
.120
.226
.318
3.834
3.760
3.548
3.364
4 4.500 .
.
STD
XS
.
.
XXS
.
.
40
80
120
160
.
5S
10S
40S
80S
.
.
.
.083
.120
.237
.337
.438
.531
.674
4.334
4.260
4.026
3.826
3.624
3.438
3.152
5 5.563 .
.
STD
XS
.
.
XXS
.
.
40
80
120
160
.
5S
10S
40S
80S
.
.
.
.109
.134
.258
.375
.500
.625
.750
5.345
5.295
5.047
4.813
4.563
4.313
4.063
6 6.625 .
.
STD
XS
.
.
XXS
.
.
40
80
120
160
.
5S
10S
40S
80S
.
.
.
.109
.134
.280
.432
.562
.718
.864
6.407
6.357
6.065
5.761
5.501
5.187
4.897
8 8.625 .
.
.
.
STD
.
XS
.
.
.
XXS
.
.
.
20
30
40
60
80
100
120
140
.
160
5S
10S
.
.
40S
.
80S
.
.
.
.
.
.109
.148
.250
.277
.322
.406
.500
.594
.719
.812
.875
.906
8.407
8.329
8.125
8.071
7.981
7.813
7.625
7.437
7.187
7.001
6.875
6.813
10 10.750 .
.
.
.
STD
XS
.
.
.
.
.
.
.
20
30
40
60
80
100
120
140
160
5S
10S
.
.
40S
80S
.
.
.
.
.
.134
.165
.250
.307
.365
.500
.594
.719
.844
1.000
1.125
10.482
10.420
10.250
10.136
10.020
9.750
9.562
9.312
9.062
8.750
8.500
12 12.75 .
.
.
.
STD
.
XS
.
.
.
.
.
.
.
.
20
30
.
40
.
60
80
100
120
140
160
5S
10S
.
.
40S
.
80S
.
.
.
.
.
.
.156
.180
.250
.330
.375
.406
.500
.562
.688
.844
1.000
1.125
1.312
12.438
12.390
12.250
12.090
12.000
11.938
11.750
11.626
11.374
11.062
10.750
10.500
10.126
14 14.00 .
.
.
.
STD
.
XS
.
.
.
.
.
..
.
.
10
20
30
40
.
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.
.
156
.188
.250
.312
.375
.438
.500
.594
.750
.938
1.094
1.250
1.406
13.688
13.624
13.500
13.376
13.250
13.124
13.000
12.812
12.500
12.124
11.812
11.500
11.188
16 16.00 .
.
.
.
STD
XS
.
.
.
.
.
.
.
.
10
20
30
40
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.
.165
.188
.250
.312
.375
.500
.656
.844
1.031
1.219
1.438
1.594
15.670
15.624
15.500
15.376
15.250
15.000
14.688
14.312
13.938
13.562
13.124
12.812
18 18.00 .
.
.
.
STD
.
XS
.
.
.
.
.
.
.
.
.
10
20
.
30
.
40
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.
.
.
.165
.188
.250
.312
.375
.438
.500
.562
.750
.938
1.156
1.375
1.562
1.781
17.670
17.624
17.500
17.376
17.250
17.124
17.000
16.876
16.500
16.124
15.688
15.250
14.876
14.438
20 20.00 .
.
.
STD
XS
.
.
.
.
.
.
.
.
.
10
20
30
40
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.
.188
.218
.250
.375
.500
.594
.812
1.031
1.281
1.500
1.750
1.969
19.624
19.564
19.500
19.250
19.000
18.812
18.376
17.938
17.438
17.000
16.500
16.062
22 22.00 .
.
.
STD
XS
.
.
.
.
.
.
.
.
10
20
30
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.188
.218
.250
.375
.500
.875
1.125
1.375
1.625
1.875
2.125
21.624
21.564
21.500
21.250
21.000
20.250
19.75
19.25
18.75
18.25
17.75
24 24.00 .
.
STD
XS
.
.
.
.
.
.
.
.
.
10
20
.
30
40
60
80
100
120
140
160
5S
10S
.
.
.
.
.
.
.
.
.
.
.218
.250
.375
.500
.562
.688
.969
1.219
1.531
1.812
2.062
2.344
23.564
23.500
23.250
23.000
22.876
22.624
22.062
21.562
20.938
20.376
19.876
19.312
26 26.00 .
STD
XS
10
.
20
.
.
.
.312
.375
.500
25.376
25.250
25.000
28 28.00 .
STD
XS
.
10
.
20
30
.
.
.
.
.312
.375
.500
.625
27.376
27.250
27.000
26.750
30 30.00 .
.
STD
XS
.
.
10
.
20
30
5S
10S
.
.
.
.250
.312
.375
.500
.625
29.500
29.376
29.250
29.000
28.750
32 32.00 .
STD
XS
.
.
10
.
20
30
40
.
.
.
.
.
.312
.375
.500
.625
.688
31.376
31.250
31.000
30.750
30.624
34 34.00 .
STD
XS
.
.
10
.
20
30
40
.
.
.
.
.
.344
.375
.500
.625
.688
33.312
33.250
33.000
32.750
32.624
36 36.00 .
STD
XS
.
.
10
.
20
30
40
.
.
.
.
.
.312
.375
.500
.625
.750
35.376
35.250
35.000
34.750
34.500
42 42.00 STD
XS
.
.
.
20
30
40
.
.
.
.
.375
.500
.625
.750
41.250
41.000
40.720
40.500

Area of Metal, Transverse Internal Area, Moment of Inertia, Weight Pipe, Weight Water, External Surface, Elastic Section Modulus

Pipe Size
(inches)
Area of Metal
(square inches)
Transverse Internal Area Moment of Inertia
- l -

(inches4)
Weight Pipe
(pounds per foot)
Weight
Water
(pounds per foot)
External Surface
(square feet per foot of pipe)
Elastic Section Modulus
(in3)
- a -
(square inches)
- A -
(square feet)
1/8 .0548
.0720
.0925
.0740
.0568
.0364
.00051
.00040
.00025
.00088
.00106
.00122
.19
.24
.31
.032
.025
.016
.106
.106
.106
.00437
.00523
.00602
1/4 .0970
.1250
.1574
.1320
.1041
.0716
.00091
.00072
.00050
.00279
.00331
.00377
.33
.42
.54
.057
.045
.031
.141
.141
.141
.01032
.01227
.01395
3/8 .1246
.1670
.2173
.2333
.1910
.1405
.00162
.00133
.00098
.00586
.00729
.00862
.42
.57
.74
.101
.083
.061
.178
.178
.178
.01736
.02160
.02554
1/2 .1583
.1974
.2503
.3200
.3836
.5043
.3959
.3568
.3040
.2340
.1706
.050
.00275
.00248
.00211
.00163
.00118
.00035
.01197
.01431
.01709
.02008
.02212
.02424
.54
.67
.85
1.09
1.31
1.71
.172
.155
.132
.102
.074
.022
.220
.220
220
.220
220
.220
.02849
.03407
.04069
.04780
.05267
.05772
3/4 .2011
.2521
.3326
.4335
.5698
.7180
.6648
.6138
.5330
.4330
.2961
.148
.00462
.00426
.00371
.00300
.00206
.00103
.02450
.02969
.03704
.04479
.05269
.05792
.69
.86
1.13
1.47
1.94
2.44
.288
.266
.231
.188
.128
.064
.275
.275
.275
.275
.275
.275
.04667
.05655
.07055
.08531
.10036
.11032
1 .2553
.4130
.4939
.6388
.8365
1.0760
1.1029
.9452
.8640
.7190
.5217
.282
.00766
.00656
.00600
.00499
.00362
.00196
.04999
.07569
.08734
.1056
.1251
.1405
.87
1.40
1.68
2.17
2.84
3.66
.478
.409
.375
.312
.230
.122
.344
.344
.344
.344
.344
.344
.07603
.11512
.1328
.1606
.1903
.2136
1 1/4 .3257
.4717
.6685
.8815
1.1070
1.534
1.839
1.633
1.495
1.283
1.057
.630
.01277
.01134
.01040
.00891
.00734
.00438
.1038
.1605
.1947
.2418
.2839
.3411
1.11
1.81
2.27
3.00
3.76
5.21
.797
.708
.649
.555
.458
.273
.435
.435
.435
.435
.435
.435
.1250
.1934
.2346
.2913
.3421
.4110
1 1/2 .3747
.6133
.7995
1.068
1.429
1.885
2.461
2.222
2.036
1.767
1.406
.950
.01709
.01543
.01414
.01225
.00976
.00660
.1579
.2468
.3099
.3912
.4824
.5678
1.28
2.09
2.72
3.63
4.86
6.41
1.066
.963
.882
.765
.608
.42
.497
.497
.497
.497
.497
.497
.1662
.2598
.3262
.4118
.5078
.5977
2 .4717
.7760
1.075
1.477
2.190
2.656
3.958
3.654
3.355
2.953
2.241
1.774
.02749
.02538
.02330
.02050
.01556
.01232
.3149
.4992
.6657
.8679
1.162
1.311
1.61
2.64
3.65
5.02
7.46
9.03
1.72
1.58
1.45
1.28
.97
.77
.622
.622
.622
.622
.622
.622
.2652
.4204
.5606
.7309
.979
1.104
2 1/2 .7280
1.039
1.704
2.254
2.945
4.028
5.764
5.453
4.788
4.238
3.546
2.464
.04002
.03787
.03322
.02942
.02463
.01710
.7100
.9873
1.530
1.924
2.353
2.871
2.48
3.53
5.79
7.66
10.01
13.69
2.50
2.36
2.07
1.87
1.54
1.07
.753
.753
.753
.753
.753
.753
.4939
.6868
1.064
1.339
1.638
1.997
3 .8910
1.274
2.228
3.016
4.205
5.466
8.730
8.347
7.393
6.605
5.408
4.155
.06063
.05796
.05130
.04587
.03755
.02885
1.301
1.822
3.017
3.894
5.032
5.993
3.03
4.33
7.58
10.25
14.32
18.58
3.78
3.62
3.20
2.6
2.35
1.80
.916
.916
.916
.916
.916
.916
.7435
1.041
1.724
2.225
2.876
3.424
3 1/2 1.021
1.463
2.680
3.678
11.545
11.104
9.886
8.888
.08017
.07711
.06870
.06170
1.960
2.755
4.788
6.280
3.48
4.97
9.11
12.50
5.00
4.81
4.29
3.84
1.047
1.047
1.047
1.047
.9799
1.378
2.394
3.140
4 1.152
1.651
3.174
4.407
5.595
6.621
8.101
14.75
14.25
12.73
11.50
10.31
9.28
7.80
.10245
.09898
.08840
.07986
.0716
.0645
.0542
2.810
3.963
7.233
9.610
11.65
13.27
15.28
3.92
5.61
10.79
14.98
19.0
22.51
27.54
6.39
6.18
5.50
4.98
4.47
4.02
3.38
1.178
1.178
1.178
1.178
1.178
1.178
1.178
1.249
1.761
3.214
4.271
5.178
5.898
6.791
5 1.868
2.285
4.300
6.112
7.953
9.696
11.340
22.44
22.02
20.01
18.19
16.35
14.61
12.97
.1558
.1529
.1390
.1263
.1136
.1015
.0901
6.947
8.425
15.16
20.67
25.73
30.03
33.63
6.36
7.77
14.62
20.78
27.04
32.96
38.55
9.72
9.54
8.67
7.88
7.09
6.33
5.61
1.456
1.456
1.456
1.456
1.456
1.456
1.456
2.498
3.029
5.451
7.431
9.250
10.796
12.090
6 2.231
2.733
5.581
8.405
10.70
13.32
15.64
32.24
31.74
28.89
26.07
23.77
21.15
18.84
.2239
.2204
.2006
.1810
.1650
.1469
.1308
11.85
14.40
28.14
40.49
49.61
58.97
66.33
7.60
9.29
18.97
28.57
36.39
45.35
53.16
13.97
13.75
12.51
11.29
10.30
9.16
8.16
1.734
1.734
1.734
1.734
1.734
1.734
1.734
3.576
4.346
8.496
12.22
14.98
17.81
20.02
8 2.916
3.941
6.57
7.26
8.40
10.48
12.76
14.96
17.84
19.93
21.30
21.97
55.51
54.48
51.85
51.16
50.03
47.94
45.66
43.46
40.59
38.50
37.12
36.46
.3855
.3784
.3601
.3553
.3474
.3329
.3171
.3018
.2819
.2673
.2578
.2532
26.44
35.41
57.72
63.35
72.49
88.73
105.7
121.3
140.5
153.7
162.0
165.9
9.93
13.40
22.36
24.70
28.55
35.64
43.39
50.95
60.71
67.76
72.42
74.69
24.06
23.61
22.47
22.17
21.70
20.77
19.78
18.83
17.59
16.68
16.10
15.80
2.258
2.258
2.258
2.258
2.258
2.258
2.258
2.258
2.258
2.258
2.258
2.258
6.131
8.212
13.39
14.69
16.81
20.58
24.51
28.14
32.58
35.65
37.56
38.48
10 4.36
5.49
8.24
10.07
11.90
16.10
18.92
22.63
26.24
30.63
34.02
86.29
85.28
82.52
80.69
78.86
74.66
71.84
68.13
64.53
60.13
56.75
.5992
.5922
.5731
.5603
.5475
.5185
.4989
.4732
.4481
.4176
.3941
63.0
76.9
113.7
137.4
160.7
212.0
244.8
286.1
324.2
367.8
399.3
15.19
18.65
28.04
34.24
40.48
54.74
64.43
77.03
89.29
104.13
115.64
37.39
36.95
35.76
34.96
34.20
32.35
31.13
29.53
27.96
26.06
24.59
2.814
2.814
2.814
2.814
2.814
2.814
2.814
2.814
2.814
2.814
2.814
11.71
14.30
21.15
25.57
29.90
39.43
45.54
53.22
60.32
68.43
74.29
12 6.17
7.11
9.82
12.87
14.58
15.77
19.24
21.52
26.03
31.53
36.91
41.08
47.14
121.50
120.57
117.86
114.80
113.10
111.93
108.43
106.16
101.64
96.14
90.76
86.59
80.53
.8438
.8373
.8185
.7972
.7854
.7773
.7528
.7372
.7058
.6677
.6303
.6013
.5592
122.4
140.4
191.8
248.4
279.3
300.3
361.5
400.4
475.1
561.6
641.6
700.5
781.1
20.98
24.17
33.38
43.77
49.56
53.52
65.42
73.15
88.63
107.32
125.49
139.67
160.27
52.65
52.25
51.07
49.74
49.00
48.50
46.92
46.00
44.04
41.66
39.33
37.52
34.89
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
3.338
19.2
22.0
30.2
39.0
43.8
47.1
56.7
62.8
74.6
88.1
100.7
109.9
122.6
14 6.78
8.16
10.80
13.42
16.05
18.66
21.21
24.98
31.22
38.45
44.32
50.07
55.63
147.15
145.78
143.14
140.52
137.88
135.28
132.73
128.96
122.72
115.49
109.62
103.87
98.31
1.0219
1.0124
.9940
.9758
.9575
.9394
.9217
.8956
.8522
.8020
.7612
.7213
.6827
162.6
194.6
255.3
314.4
372.8
429.1
483.8
562.3
678.3
824.4
929.6
1027.0
1117.0
23.07
27.73
36.71
45.61
54.57
63.44
72.09
85.05
106.13
130.85
150.79
170.28
189.11
63.77
63.17
62.03
60.89
59.75
58.64
57.46
55.86
53.18
50.04
47.45
45.01
42.60
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
3.665
23.2
27.8
36.6
45.0
53.2
61.3
69.1
80.3
98.2
117.8
132.8
146.8
159.6
16 8.21
9.34
12.37
15.38
18.41
24.35
31.62
40.14
48.48
56.56
65.78
72.10
192.85
191.72
188.69
185.69
182.65
176.72
169.44
160.92
152.58
144.50
135.28
128.96
1.3393
1.3314
1.3103
1.2895
1.2684
1.2272
1.1766
1.175
1.0596
1.0035
.9394
.8956
257.3
291.9
383.7
473.2
562.1
731.9
932.4
1155.8
1364.5
1555.8
1760.3
1893.5
27.90
31.75
42.05
52.27
62.58
82.77
107.50
136.61
164.82
192.43
223.64
245.25
83.57
83.08
81.74
80.50
79.12
76.58
73.42
69.73
66.12
62.62
58.64
55.83
4.189
4.189
4.189
4.189
4.189
4.189
4.189
4.189
4.189
4.189
4.189
4.189
32.2
36.5
48.0
59.2
70.3
91.5
116.6
144.5
170.5
194.5
220.0
236.7
18 9.25
10.52
13.94
17.34
20.76
24.17
27.49
30.79
40.64
50.23
61.17
71.81
80.66
90.75
245.22
243.95
240.53
237.13
233.71
230.30
226.98
223.68
213.83
204.24
193.30
182.66
173.80
163.72
1.7029
1.6941
1.6703
1.6467
1.6230
1.5990
1.5763
1.5533
1.4849
1.4183
1.3423
1.2684
1.2070
1.1369
367.6
417.3
549.1
678.2
806.7
930.3
1053.2
1171.5
1514.7
1833.0
2180.0
2498.1
2749.0
3020.0
31.43
35.76
47.39
58.94
70.59
82.15
93.45
104.67
138.17
170.92
207.96
244.14
274.22
308.50
106.26
105.71
104.21
102.77
101.18
99.84
98.27
96.93
92.57
88.50
83.76
79.07
75.32
70.88
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
4.712
40.8
46.4
61.1
75.5
89.6
103.4
117.0
130.1
168.3
203.8
242.3
277.6
305.5
335.6
20 11.70
13.55
15.51
23.12
30.63
36.15
48.95
61.44
75.33
87.18
100.33
111.49
302.46
300.61
298.65
290.04
283.53
278.00
265.21
252.72
238.83
226.98
213.82
202.67
2.1004
2.0876
2.0740
2.0142
1.9690
1.9305
1.8417
1.7550
1.6585
1.5762
1.4849
1.4074
574.2
662.8
765.4
1113.0
1457.0
1703.0
2257.0
2772.0
3315.2
3754.0
4216.0
4585.5
39.78
46.06
52.73
78.60
104.13
123.11
166.40
208.87
256.10
296.37
341.09
379.17
131.06
130.27
129.42
125.67
122.87
120.46
114.92
109.51
103.39
98.35
92.66
87.74
5.236
5.236
5.236
5.236
5.236
5.236
5.236
5.236
5.236
5.236
5.236
5.236
57.4
66.3
75.6
111.3
145.7
170.4
225.7
277.1
331.5
375.5
421.7
458.5
22 12.88
14.92
17.08
25.48
33.77
58.07
73.78
89.09
104.02
118.55
132.68
367.25
365.21
363.05
354.66
346.36
322.06
306.35
291.04
276.12
261.59
247.45
2.5503
2.5362
2.5212
2.4629
2.4053
2.2365
2.1275
2.0211
1.9175
1.8166
1.71840
766.2
884.8
1010.3
1489.7
1952.5
3244.9
4030.4
4758.5
5432.0
6053.7
6626.4
43.80
50.71
58.07
86.61
114.81
197.41
250.81
302.88
353.61
403.00
451.06
159.14
158.26
157.32
153.68
150.09
139.56
132.76
126.12
119.65
113.36
107.23
5.760
5.760
5.760
5.760
5.760
5.760
5.760
5.760
5.760
5.760
5.760
69.7
80.4
91.8
135.4
117.5
295.0
366.4
432.6
493.8
550.3
602.4
24 16.29
18.65
27.83
36.91
41.39
50.31
70.04
87.17
108.07
126.31
142.11
159.41
436.10
433.74
424.56
415.48
411.00
402.07
382.35
365.22
344.32
326.08
310.28
292.98
3.0285
3.0121
2.9483
2.8853
2.8542
2.7921
2.6552
2.5362
2.3911
2.2645
2.1547
2.0346
1151.6
1315.4
1942.0
2549.5
2843.0
3421.3
4652.8
5672.0
6849.9
7825.0
8625.0
9455.9
55.37
63.41
94.62
125.49
140.68
171.29
238.35
296.58
367.39
429.39
483.12
542.13
188.98
187.95
183.95
179.87
178.09
174.23
165.52
158.26
149.06
141.17
134.45
126.84
6.283
6.283
6.283
6.283
6.283
6.283
6.283
6.283
6.283
6.283
6.283
6.283
96.0
109.6
161.9
212.5
237.0
285.1
387.7
472.8
570.8
652.1
718.9
787.9
26 25.18
30.19
40.06
505.75
500.74
490.87
3.5122
3.4774
3.4088
2077.2
2478.4
3257.0
85.60
102.63
136.17
219.16
216.99
212.71
6.806
6.806
6.806
159.8
190.6
250.5
28 27.14
32.54
43.20
53.75
588.61
583.21
572.56
562.00
4.0876
4.0501
3.9761
3.9028
2601.0
3105.1
4084.8
5037.7
92.26
110.64
146.85
182.73
255.07
252.73
248.11
243.53
7.330
7.330
7.330
7.330
185.8
221.8
291.8
359.8
30 23.37
29.10
34.90
46.34
57.68
683.49
677.76
671.96
660.52
649.18
4.7465
4.7067
4.6664
4.5869
4.5082
2585.2
3206.3
3829.4
5042.2
6224.0
79.43
98.93
118.65
157.53
196.08
296.18
293.70
291.18
286.22
281.31
7.854
7.854
7.854
7.854
7.854
172.3
213.8
255.3
336.1
414.9
32 31.06
37.26
49.48
61.60
67.68
773.19
766.99
754.77
742.64
736.57
5.3694
5.3263
5.2414
5.1572
5.1151
3898.9
4658.5
6138.6
7583.4
8298.3
105.59
126.66
168.21
209.43
230.08
335.05
332.36
327.06
321.81
319.18
8.378
8.378
8.378
8.378
8.378
243.7
291.2
383.7
474.0
518.6
34 36.37
39.61
52.62
65.53
72.00
871.55
868.31
855.30
842.39
835.92
6.0524
6.0299
5.9396
5.8499
5.8050
5150.5
5599.3
7383.5
9127.6
9991.6
123.65
134.67
178.89
222.78
244.77
377.67
376.27
370.63
365.03
362.23
8.901
8.901
8.901
8.901
8.901
303.0
329.4
434.3
536.9
587.7
36 34.98
41.97
55.76
69.46
83.06
982.90
975.91
962.11
948.42
934.82
6.8257
6.7771
6.6813
6.5862
6.4918
5569.5
6658.9
8786.2
10868.4
12906.1
118.92
142.68
189.57
236.13
282.35
425.92
422.89
416.91
417.22
405.09
9.425
9.425
9.425
9.425
9.425
309.4
369.9
488.1
603.8
717.0
42 49.08
65.18
81.28
97.23
1336.3
1320.2
1304.1
1288.2
.
.
.
.
10627
14037
17373
20689
167
222
276
330
579.3
572.3
565.4
558.4
10.99
10.99
10.99
10.99
506.1
668.4
827.3
985.2

STD, XS and XXS

To distinguish different weights of pipe, three long standing traditional designations are used:

The last two designations are sometimes referred to as extra heavy wall (XH), and double extra heavy wall (XXH).

Sponsored Links

Related Topics

  • Piping Systems Dimensions of pipes and tubes - dimensions, materials, capacities - pressure drop calculations and charts - insulation and heat loss diagrams
  • Dimensions Sizes and dimensions of pipes and tubes, and their fittings - inside and outside diameter, weight and more

Related Documents

Sponsored Links



Engineering ToolBox - SketchUp Edition - Online 3D modeling!

Engineering ToolBox - SketchUp Edition - enabled for use with the amazing, fun and free Google SketchUp.


Search the ToolBox

Google
Web The Engineering ToolBox

© The Engineering ToolBox 2005

9 6 19

handheld Engineering ToolBox - optimized for mobile devices! 3D Engineering ToolBox - draw and model technical applications!


.
Resources, Tools and Basic Information  for Engineering and Design of Technical Applications!

Resources, Tools and Basic Information for Engineering and Design of Technical Applications!