Dimensions of stainless steel weld fittings according ANSI/ASME 36.19M Stainless Steel Pipe can be found in the tables below.
Note! Wall thickness and weights are different for different stainless steel schedules.
| Nominal Pipe Size (inches) |
Outside Diameter |
90o Elbows | 45o Elbows | 180o Returns | ||||
| Long Radius | Short Radius | Long Radius | Long Radius | |||||
| (mm) | (inches) | Center to Face (inches) |
Center to Face (inches) |
Center to Face (inches) |
Radius (inches) |
Center to Center (inches) |
Back to face (inches) |
|
| 1/2 | 21.3 | 0.840 | 1 1/2 | - | 5/8 | 2 | 1 7/8 | |
| 3/4 | 26.7 | 1.050 | 1 1/8 | - | 7/16 | 2 1/4 | 1 11/16 | |
| 1 | 33.4 | 1.315 | 1 1/2 | 1 | 7/8 | 3 | 2 3/16 | |
| 1 1/4 | 42.2 | 1.660 | 1 7/8 | 1 1/4 | 1 | 3 3/4 | 2 3/4 | |
| 1 1/2 | 48.3 | 1.900 | 2 1/4 | 1 1/2 | 1 1/8 | 3 | 4 1/2 | 3 1/4 |
| 2 | 60.3 | 2.375 | 3 | 2 | 1 3/8 | 4 | 6 | 4 3/16 |
| 2 1/2 | 73.0 | 2.875 | 3 3/4 | 2 1/2 | 1 3/4 | 5 | 7 1/2 | 5 3/16 |
| 3 | 88.9 | 3.500 | 4 1/2 | 3 | 2 | 6 | 9 | 6 1/4 |
| 3 1/2 | 101.6 | 4.000 | 5 1/4 | 3 1/2 | 2 1/4 | 7 | 10 1/2 | 7 1/4 |
| 4 | 114.3 | 4.500 | 6 | 4 | 2 1/2 | 8 | 12 | 8 1/4 |
| 5 | 141.3 | 5.563 | 7 1/2 | 5 | 3 1/8 | 10 | 15 | 10 5/16 |
| 6 | 168.3 | 6.625 | 9 | 6 | 3 3/4 | 12 | 18 | 12 5/16 |
| 8 | 219.1 | 8.625 | 12 | 8 | 5 | 12 | 24 | 16 5/16 |
| 10 | 273.1 | 10.750 | 15 | 10 | 6 1/4 | 15 | 30 | 20 3/8 |
| 12 | 323.9 | 12.750 | 18 | 12 | 7 1/2 | 18 | 36 | 24 3/8 |
| Nominal Pipe Size (inches) |
Outside Diameter |
Caps | Straight Tees | Straight Crosses | Stub Ends | |||
| (mm) | (inches) | Length (inches) |
Center to End (inches) |
Center to End (inches) |
Lap Diameter (inches) |
Long Length (inches) |
Short Length (inches) |
|
| 1/2 | 21.3 | 0.840 | 1 | 1 | - | 1 3/8 | 3 | 2 |
| 3/4 | 26.7 | 1.050 | 1 | 1 1/8 | - | 1 11/16 | 3 | 2 |
| 1 | 33.4 | 1.315 | 1 1/2 | 1 1/2 | 1 1/2 | 2 | 4 | 2 |
| 1 1/4 | 42.2 | 1.660 | 1 1/2 | 1 7/8 | 1 7/8 | 2 1/2 | 4 | 2 |
| 1 1/2 | 48.3 | 1.900 | 1 1/2 | 2 1/4 | 2 1/4 | 2 7/8 | 4 | 2 |
| 2 | 60.3 | 2.375 | 1 1/2 | 2 1/2 | 2 1/2 | 3 5/8 | 6 | 2 1/2 |
| 2 1/2 | 73.0 | 2.875 | 1 1/2 | 3 | 3 | 4 1/8 | 6 | 2 1/2 |
| 3 | 88.9 | 3.500 | 2 | 3 3/8 | 3 3/8 | 5 | 6 | 2 1/2 |
| 3 1/2 | 101.6 | 4.000 | 2 1/2 | 3 3/4 | 3 3/4 | 5 1/2 | 6 | 3 |
| 4 | 114.3 | 4.500 | 2 1/2 | 4 1/8 | 4 1/8 | 6 3/16 | 6 | 3 |
| 5 | 141.3 | 5.563 | 3 | 4 7/8 | 4 7/8 | 7 5/16 | 8 | 3 |
| 6 | 168.3 | 6.625 | 3 1/2 | 5 5/8 | 5 5/8 | 8 1/2 | 8 | 3 1/2 |
| 8 | 219.1 | 8.625 | 4 | 7 | 7 | 10 5/8 | 8 | 4 |
| 10 | 273.1 | 10.750 | 5 | 8 1/2 | 8 1/2 | 12 3/4 | 10 | 5 |
| 12 | 323.9 | 12.750 | 6 | 10 | 10 | 15 | 10 | 6 |
| Nominal Pipe Size |
Outside Diameter |
Reducers | ||
| Reduced from (inches) |
(mm) | (inches) | Reduced to (inches) |
Concentric & Eccentric Length (inches) |
| 1/2 | 21.3 | 0.840 | 1/4 | 1 1/2 |
| 3/8 | 1 1/2 | |||
| 3/4 | 26.7 | 1.050 | 3/8 | 2 |
| 1/2 | 2 | |||
| 1 | 33.4 | 1.315 | 3/8 | 2 |
| 1/2 | 2 | |||
| 3/4 | 2 | |||
| 1 1/4 | 42.2 | 1.660 | 1/2 | 2 |
| 3/4 | 2 | |||
| 1 | 2 | |||
| 1 1/2 | 48.3 | 1.900 | 1/2 | 2 1/2 |
| 3/4 | 2 1/2 | |||
| 1 | 2 1/2 | |||
| 1 1/4 | 2 1/2 | |||
| 2 | 60.3 | 2.375 | 3/4 | 3 |
| 1 | 3 | |||
| 1 1/4 | 3 | |||
| 1 1/2 | 3 | |||
| 2 1/2 | 73.0 | 2.875 | 1 | 3 1/2 |
| 1 1/4 | 3 1/2 | |||
| 1 1/2 | 3 1/2 | |||
| 2 | 3 1/2 | |||
| 3 | 88.9 | 3.500 | 1 | 3 1/2 |
| 1 1/2 | 3 1/2 | |||
| 2 | 3 1/2 | |||
| 2 1/2 | 3 1/2 | |||
| 3 1/2 | 101.6 | 4.000 | 1 1/4 | 4 |
| 1 1/2 | 4 | |||
| 2 | 4 | |||
| 2 1/2 | 4 | |||
| 3 | 4 | |||
| 4 | 114.3 | 4.500 | 1 1/2 | 4 |
| 2 | 4 | |||
| 2 1/2 | 4 | |||
| 3 | 4 | |||
| 3 1/2 | 4 | |||
| 5 | 141.3 | 5.563 | 2 | 5 |
| 2 1/2 | 5 | |||
| 3 | 5 | |||
| 3 1/2 | 5 | |||
| 4 | 5 | |||
| 6 | 168.3 | 6.625 | 2 1/2 | 5 1/2 |
| 3 | 5 1/2 | |||
| 3 1/2 | 5 1/2 | |||
| 4 | 5 1/2 | |||
| 5 | 5 1/2 | |||
| 8 | 219.1 | 8.625 | 3 | 6 |
| 3 1/2 | 6 | |||
| 4 | 6 | |||
| 5 | 6 | |||
| 6 | 6 | |||
| 10 | 273.1 | 10.750 | 4 | 7 |
| 5 | 7 | |||
| 6 | 7 | |||
| 8 | 7 | |||
| 12 | 323.9 | 12.750 | 5 | 8 |
| 6 | 8 | |||
| 8 | 8 | |||
| 10 | 8 | |||