Molybdenum Binary Eutectic Alloys - Melting Points
Mo - Molybdenum - binary eutectic alloys and melting points.
The melting point of an alloy of two (binary) or more metals depends on the relative proportions of the ingredients.
- an eutectic mixture is the mixture where the melting point is as low as possible
Binary eutectic Molybdenum - Mo - alloys, with composition and melting points are indicated below:
| Alloy Component | Weight of Alloy Component (%) | Melting Point | |
|---|---|---|---|
| K | oF | ||
| Nb - Niobium (Columbium) | 65 | 2570 | 4167 |
| Ni - Nickel | 52 | 1590 | 2403 |
| Os - Osmium | 34 | 2650 | 4311 |
| Pd - Palladium | 57 | 2020 | 3177 |
| Re - Rhenium | 64 | 2780 | 4545 |
| Ru - Ruthenium | 42 | 2200 | 3501 |
| Si - Silicon | 5.7 | 2350 | 3771 |
- T (oC) = 5/9 (T (oF) - 32)