The Engineering ToolBox Web Google

Hydrostatic Test Pressure Flanges

Flanged fittings and hydrostatic test pressure

Sponsored Links

Hydrostatic test pressure for flanged fittings in some common piping materials are indicated in the table below:

Hydrostatic Test Pressure (psig)
ASTM
Specification
Class
150 300 400 600 900 1500 2500
A105
A216-WCB
A350-LF2
A515-70
A516-70
A537-C1.1
A675-70
A672-B70
A672-C70
A696 Grade C
450 1125 1500 2225 3350 5575 9275
A106-C
A203-B
A203-E
A216-WCC
A350-LC3
A352-LCC
A352-LC2
A352-LC3
450 1125 1500 2250 3375 5625 9375
A203-A
A203-D
A352-LCB
A515-65
A516-65
A675-65
A672-B65
A672-C65
400 1050 1400 2100 3150 5225 8700
A106-B
A350-LF1
A515-60
A516-60
A672-B60
A672-C60
A675-60
A696 Grade B
375 950 1250 1875 2775 4650 7725
A182-F1
A204-A
A204-B
A217-WC1
A352-LC1
A691-CM70
400 1050 1400 2100 3150 5225 8700
A182-F2
A204-C
A217-WC4
A217-WC5
A691-CM75
450 1125 1500 2250 3375 5625 9375
A182-F12
A182-F11
A217-WC6
A387-11C1.2
A739-B11
450 1125 1500 2250 3375 5625 9375
A182-F304
A182-F304H
A240-304
A240-304H
A312-TP304
A312-TP304H
A351-CF3
A351-CF8
A479-304
A479-304H
425 1100 1450 2175 3250 5400 9000

Sponsored Links

Related Topics

  • Pressure Ratings Pressure ratings of pipes and tubes and their fittings - carbon steel , stainless steel, plastic, copper and more

Related Documents

Sponsored Links



Engineering ToolBox - SketchUp Edition - Online 3D modeling!

Engineering ToolBox - SketchUp Edition - enabled for use with the amazing, fun and free Google SketchUp.


Search the ToolBox

Google
Web The Engineering ToolBox

© The Engineering ToolBox 2005

9 11 11

handheld Engineering ToolBox - optimized for mobile devices! 3D Engineering ToolBox - draw and model technical applications!


.